We report the thermoelectric properties of Bi2Te3 thin films electrodeposited from the weakly coordinating solvent dichloromethane (CH2Cl2). It was found that the oxidation of porous films is significant, causing the degradation of its thermoelectric properties. We show that the morphology of the film can be improved drastically by applying a short initial nucleation pulse, which generates a large number of nuclei, and then growing the nuclei by pulsed electrodeposition at a much lower overpotential. This significantly reduces the oxidation of the films as smooth films have a smaller surface-to-volume ratio and are less prone to oxidation. X-ray photoelectron spectroscopy (XPS) shows that those films with Te(O) termination show a complete absence of oxygen below the surface layer. A thin film transfer process was developed using polystyrene as a carrier polymer to transfer the films from the conductive TiN to an insulating layer for thermoelectrical characterization. Temperature-dependent Seebeck measurements revealed a room-temperature coefficient of −51.7 μV/K growing to nearly −100 μV/K at 520 °C. The corresponding power factor reaches a value of 88.2 μW/mK2 at that temperature.
We herein report the results of a facile two-step surfactant assisted reflux synthesis of bismuth telluride (Bi2Te3) nanowires (NWs). The as-synthesised NWs had diameters ranging from 70 to 110 nm with a length varying between 0.4 and 3 µm and a preferential lattice orientation of (0 1 5) as determined by grazing incidence x-ray diffraction. We demonstrate for the first time that a solvent/binder paste formulation of N-methyl-2-pyrrolidone/polyvinylidene fluoride (PVDF) is suitable for screen-printing the Bi2Te3 NWs with the potential for the fabrication of flexible thermoelectric (TE) materials. The wt% of PVDF in the composite films was varied from 10% to 20% to identify the optimal composition with a view to achieving maximum film flexibility whilst retaining the best TE performance. The films were screen-printed onto Kapton substrates and subjected to a post-printing annealing process to improve TE performance. The annealed and screen printed Bi2Te3/PVDF NW composites yielded a maximum Seebeck coefficient −192 µV K−1 with a power factor of 34 µW m−1K−2 at 225 K. The flexible screen printed composite films were flexible and found to be intact even after 2000 bending cycles.
[nBu3Sn(TenBu)] is an effective precursor for the low temperature growth of continuous SnTe thin films by low pressure CVD; temperature-dependent thermoelectric characterisation of these p-type films is reported.