This paper assesses the workability and strength properties of alkali activated mortar produced using silicomanganese fume (AASiMnF) as a sole binder (source material) with alkaline activators and sand cured at room temperature (23 ± 1 °C). A total of 18 mixtures were prepared by varying binder content (370 kg/m3, 470 kg/m3 and 570 kg/m3), alkaline activator content (33%, 43% and 53% of binder by weight) and NaOH concentration (8M and 12M). Scanning electron microscopy (SEM), X-ray diffraction (XRD) and Fourier-transform infrared spectroscopy (FTIR) techniques were utilized to study the morphology, mineral composition and functional groups formed, respectively in the developed AASiMnF paste (AAP). Statistical modeling, including analysis of variance (ANOVA) and response surface method (RSM) was undertaken to optimize the mixes and life cycle assessment was also done to assess the environmental impact of the developed AASiMnF based mortar. The flow of mortar increased with the increase in the percentage of alkaline activator. Based on the strength and flow results, the mix having 470 kg/m3 of SiMnF and 43% alkaline activator content of concentration of 8-12M NaOH was found to give the maximum strength. AASiMnF mixes had better workability and mechanical properties when prepared and cured at room temperature thereby making it adaptive to real life applications.