Zhengning Li

Zhengning Li

Auto-generated profile, based on publicly available information

Zhengning Li

School of Materials Science and Engineering, Lanzhou Jiaotong University, Lanzhou, China

Research Focus & Metrics

Academic Career Length

26Years (2001-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 January 2001 in Journal of Molecular Catalysis A: Chemical
Verified
Journal Article
Closed access
ZLZhengning Li
Zhengning Li
ZZZhuo Zheng
Zhuo Zheng
BWBoshun Wan
Boshun Wan
HCHuilin Chen
Huilin Chen

16 September 2024 in Materials
Verified
Journal Article
Open access
PDF file
ZMZhonglei Ma
Zhonglei Ma
HWHongding Wang Hongding Wang
Hongding Wang Hongding Wang
YZYanlong Zhao
Yanlong Zhao
ZLZhengning Li
Zhengning Li
HLHong Liu
Hong Liu
ZZZigeng Zhao
Zigeng Zhao
This study explores the mechanical properties of graphene/aluminum (Gr/Al) nanocomposites through nanoindentation testing performed via molecular dynamics simulations in a large-scale atomic/molecular massively parallel simulator (LAMMPS). The simulation model was initially subjected to energy minimization at 300 K, followed by relaxation for 50 ps under the NPT ensemble, wherein the number of atoms (N), simulation temperature (T), and pressure (P) were conserved. After the model was fully relaxed, loading and unloading simulations were performed. This study focused on the effects of the Gr arrangement with a brick-and-mortar structure and incorporation of high-entropy alloy (HEA) coatings on mechanical properties. The findings revealed that Gr sheets (GSs) significantly impeded dislocation propagation, preventing the dislocation network from penetrating the Gr layer within the plastic zone. However, interactions between dislocations and GSs in the Gr/Al nanocomposites resulted in reduced hardness compared with that of pure aluminum. After modifying the arrangement of GSs and introducing HEA (FeNiCrCoAl) coatings, the elastic modulus and hardness of the Gr/Al nanocomposites were 83 and 9.5 GPa, respectively, representing increases of 21.5% and 17.3% compared with those of pure aluminum. This study demonstrates that vertically oriented GSs in combination with HEA coatings at a mass fraction of 3.4% significantly enhance the mechanical properties of the Gr/Al nanocomposites.

29 January 2022 in Coatings
Verified
Journal Article
Open access
PDF file
WWWenke Wang
Wenke Wang
YGYang Guo
Yang Guo
YLYuanbo Li
Yuanbo Li
ZLZhengning Li
Zhengning Li
This study systematically evaluated the fracture toughness of a CrMoV/NiCrMoV dissimilar metal welded joint (DMWJ) with buttering layer technology in a steam turbine rotor. The fracture resistance curves and parameters of base metals (BM-1 and BM-2), weld metal (WM), buttering layer (BL), and heat-affected zones (HAZ-1 and HAZ-2) in the welded joint were all obtained. The characteristic microstructures, carbides, and fracture surfaces were observed by optical microscopy (OM), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The results revealed a different fracture toughness of each region in the DMWJ. The BM-1 showed a brittle fracture mode, mainly related to the directional needle-shaped carbide M3C. However, HAZ-1, BL, WM, HAZ-2, and BM-2 illustrated ductile fracture mode. The tempered microstructure and dispersed carbides increased the toughness of each material. Except for BM-1, the ductile fracture toughnesses of BL and WM were low in DMWJ due to coarse spherical carbide M7C3. The fracture toughness in the middle of HAZs was higher than that of the corresponding BMs owing to the fine tempered martensite and bainite. The fracture toughness along DMWJ appeared uneven. In sum, these findings look promising for the accurate integrity evaluation of DMWJs.

29 January 2017 in Advances in Materials Science and Engineering
Verified
Journal Article
Open access
PDF file
ZLZhengning Li
Zhengning Li
FWFuan Wei
Fuan Wei
PLPeiqing La
Peiqing La
HWHongding Wang Hongding Wang
Hongding Wang Hongding Wang
YWYupeng Wei
Yupeng Wei
The 1045 steel with lamellar spacing of pearlite in nanometer was prepared by aluminothermic reaction casting and annealed at 873 K (600°C) with different time. Microstructures of steels were investigated by X-ray diffraction (XRD), scanning electron microscope (SEM), and transmission electron microscope (TEM). Tensile properties of the steels were measured. The results showed that the lamellar spacing of the pearlite increased with the annealing time. It was found that the microstructure of steels consisted of nanocrystalline-ferrite matrix and laminar pearlite phase. The average grain sizes of the ferrite were 26.9, 27.0, 26.1, and 34.9 nm for the cast steel and samples annealed for 2, 4, and 6 h, respectively. As the annealing time increased, the volume fraction of the pearlite almost remained constant, while the laminar spacing of pearlite increased from 146 to 300 nm. The tensile and yield strength varied slightly; the elongation obviously improved. After annealing for 4 h, the elongation increased to be 33%, which was the reported highest value for the steel up to now and about twice of the conventional 1045 steel.

30 October 2017 in Steel Research International
Verified
Journal Article
Closed access
PDF file
ZLZhengning Li
Zhengning Li
BSBo Shi
Bo Shi
PLPeiqing La
Peiqing La
JSJie Sheng
Jie Sheng

1 August 2021 in Materials Research Express
Verified
Journal Article
Open access
ZLZhengning Li
Zhengning Li
PLPeiqing La
Peiqing La
FWFuan Wei
Fuan Wei
A heterogeneous structural (HS) 1045 steel prepared by aluminothermic reaction (AR) casting method was fabricated by combining severe deformation cold rolled with subsequently heating. Its detailed microstructure evolution, mechanical properties, strengthening and toughening mechanisms were investigated. The heterogeneous structure (HS) is characterized with trimodal grain size distribution of ferrite (with microcrystalline grain sizes of >1000 nm, ultrafine grain sizes of ∼1000 nm, nanocrystalline grain sizes of ∼100 nm grains, respectively) and cementite nanoparticles (with particle sizes of 11∼120 nm). The HS 1045 steel shows an outstanding strength-ductility synergy. When the cold rolled steel was heated at 400 °C with 1 h, comparing with casting steel, the yield strength and tensile strength increased by 87.4% and 35%, to 1420 and 1602 MPa, respectively, and surprisingly, the ductility was only with a small sacrifice, the elongation rate is maintained at the level of 10.6%. The improved strength is mainly attributed to multiple strengthening mechanisms, fine-grain strengthening, cementite nanoparticles strengthening, dislocation strengthening, and solution strengthening. The reasonable ductility can be attributed to the heterogeneous structure, as it can offer an extra work hardening ability introduced by generation of geometrically necessary dislocations (GNDs) near heterointerfaces.