5 April 2017 in Oxidation of Metals
Investigations into potentially extending the lives of UK advanced gas-cooled reactors have highlighted the need for improved understanding of the long-term oxidation and carburisation of 9Cr ferritic steels. These steels were used in evaporators and primary superheaters and as these are to be used beyond their original design lives, it is necessary to ensure that these degradation routes remain within acceptable levels. A dimensional metrology technique has been applied to archived autoclave samples to measure such damage. These samples had previously been exposed to a range of temperatures, pressures and gas chemistries representative of those experienced by 9Cr steels in CO2-rich AGR gases. Earlier sample assessments had focused on weight change measurements, but the dimensional technique enables measurement of duplex oxide thicknesses around samples and the extraction of related data from longer exposure times. These data also support estimation of the extent of both carbon and oxygen uptake.
1 October 2021 in Corrosion Science
19 October 2017 in Materials at High Temperatures
EDF Energy operates 14 advanced gas cooled reactors (AGRs) in the UK to generate electricity. CO2 gas is used as the primary coolant in the AGRs, and a range of steels are used as for the structural components: e.g. 9Cr-1Mo ferritic steels and stainless steels. These steels are susceptible to both oxidation and carburisation in CO2 dominated primary coolant gas under high pressure between 300 and 650 °C. Material degradation is a key concern for lifetime extension of the power stations, and EDF Energy and its predecessors have carried out a series of research programmes to better understand steel oxidation behaviour in AGRs and to develop more realistic lifetime prediction methodologies. These are used to secure safe and reliable operation of the AGRs. In this paper, an overview of oxidation behaviour of steels used in AGRs and some examples from the above programmes are described.