30 July 2025 in Batteries & Supercaps
Understanding charge compensation mechanisms in nickel‐rich lithium nickel–manganese–cobalt alloy oxide (NMC) cathodes is crucial for optimizing their electrochemical performance. This study employs complementary spectroscopic techniques with varying probing depths, including X‐ray absorption near‐edge structure spectroscopy, hard X‐ray photoemission spectroscopy, X‐ray photoelectron spectroscopy, and ion beam analysis, to investigate the correlation between transition metal oxidation states and Li depth profile in NMC811. This approach reveals different charge compensation mechanisms depending on the local Li content, which exhibits near‐surface gradients. The results show that Ni oxidation is the main charge compensation mechanism for moderate delithiations at a Li stoichiometry x > 0.35. When the Li content drops below the threshold x = 0.3, which occurs near the surface for high state of charge (SOC), compensation by Ni/Li mixing prevails. Meanwhile, the Li‐depleted surface (with x ≪ 0.3) shows evidence of transformation into electrochemically inactive Li‐free cubic phases. The voltage window used to cycle the NMC811 prevents the bulk Li content from falling below x = 0.35, so the different charge compensation mechanisms coexist for high SOCs, allowing to compare between their kinetics. This study contributes to a comprehensive understanding of the electrochemical behavior of nickel‐rich NMCs, aiding the development of high‐energy Li‐ion batteries with improved stability.
29 December 2025 in Battery Energy
Metal components are extensively used as current collectors, anodes, and interlayers in lithium‐ion batteries. Integrating these functions into one component enhances the cell's energy density and simplifies its design. However, this multifunctional component must meet stringent requirements, including high and reversible Li storage capacity, rapid lithiation/delithiation kinetics, mechanical stability, and safety. Six single‐atom metals (Mg, Zn, Al, Ag, Sn, and Cu) are screened for lithiation behavior through their interaction with ion beams in electrochemically tested samples subjected to both weak and strong lithiation regimes. These different lithiation regimes allowed us to differentiate between the thermodynamics and kinetic aspects of the lithiation process. Three types of ions are used to determine Li depth profile: H + for nuclear reaction analysis (NRA), He + for Rutherford backscattering (RBS), and Ga + for focused ion beam milling. The study reveals three lithiation behaviors: (i) Zn, Al, Sn form pure alloys with Li; (ii) Mg, Ag create intercalation solid solutions; (iii) Cu acts as a lithiation barrier. NRA and RBS offer direct and quantitative data, providing a more comprehensive understanding of the lithiation process in LIB components. These findings fit well with our ab initio simulation results, establishing a direct correlation between electrochemical features and fundamental thermodynamic parameters.
19 August 2026 in ACS Applied Materials & Interfaces
The dependence of practicable lithium-storage capacity on the charge–discharge rate is crucial for deploying lithium-ion batteries in energy-intensive applications that demand high current densities and short recharge times. Under high-current operation, where most electrode materials fail, Ag stands out as a benchmark for systems where metal electrodes function both as an anode and current collector, increasing its practicable capacity at elevated rates. This performance arises from the rapid formation of γ-brass-type alloy phases, which enable intercalation-solid-solution-like lithium storage with fast kinetics, high capacity, and suppressed lithium loss even at high rates. This behavior is directly resolved by combining electrochemistry with ion beam analysis, which provides quantitative lithium concentration profiles and depth-resolved coulombic efficiency across current densities. The results reveal that Ag maintains efficient lithium utilization by minimizing irreversible trapping and surface-driven loss pathways. In contrast, Mg and Al exhibit pronounced rate-dependent irreversibility due to diffusion-limited lithiation and Li trapping in structural defects, while Cu shows the most severe degradation, dominated by porous, highly reactive Li plating. These findings establish Ag as a model system for high-rate metal electrodes and demonstrate that controlling lithiation behavior is key to enabling stable anode-free battery operation under demanding conditions.