Photocatalytic reduction of CO2 into C2,3 hydrocarbons completes a C‐neutral cycle. The reaction pathways of photocatalytic generation of C2,3 paraffin and C2H4 from CO2 are mostly unclear. Herein, a Co0−ZrO2 photocatalyst converted CO2 into C1–3 paraffin, while selectively converting CO into C2H4 and C3H6 (6.0±0.6 μmol h−1 gcat−1, 70 mol %) only under UV/Visible light. The photocatalytic cycle was conducted under 13CO and H2, with subsequent evacuation and flushing with CO. This iterative process led to an increase in the population of C2H4 and C3H6 up to 61–87 mol %, attributed to the accumulation of CH2 species at the interface between Co0 nanoparticles and the ZrO2 surface. CO2 adsorbed onto the O vacancies of the ZrO2 surface, with resulting COH species undergoing hydrogenation on the Co0 surface to yield C1–3 paraffin using either H2 or H2O (g, l) as the reductant. In contrast, CO adsorbed on the Co0 surface, converted to HCOH species, and then split into CH and OH species at the Co and O vacancy sites on ZrO2, respectively. This comprehensive study elucidates intricate photocatalytic pathways governing the transformation of CO2 into paraffin and CO to olefins.
1 July 2021 in The Journal of Physical Chemistry C
A SEI (Solid Electrolyte Interphase) is formed on the surface layer of the negative electrode active material of a lithium ion secondary battery (LIB) during the initial charging process, and its morphology and structure significantly affect performance and safety. In this study, by conducting ex situ experiments, SEM, TEM and STEM-EELS observations were performed on Si negative electrodes under charge state within an actual battery and Si negative electrodes directly charged on a TEM thin film, revealed morphology and structure of the SEI. All of the processes from specimen preparation for electron microscopy observation to specimen transport were performed under non-atmospheric exposure conditions.The SEI on the surface of the Si negative electrode grew thicker as the charge depth increased. On the other hands, LixSi amorphous phase due to the lithiation by solid-state reaction was confirmed inside the Si negative electrode. It was found that Li2O was formed on the most surface of the Si negative electrode at the initial stage of charging, and the SEI was mainly composed of Li2O. The SEI of about 1 µm was observed on the Si negative electrode after 40% charge, and the thickness of the SEI decreased to less than 1/5 after discharge. This Paper was Originally Published in Japanese in Japan Inst. Met. Mater. 84 (2020) 382–390.