8 June 2012 in Optics Letters
High-power supercontinuum spanning over more than an octave was generated using a high power femtosecond fiber laser amplifier and a multicore nonlinear photonic crystal fiber (PCF). Long multicore PCFs (as long as 20 m in our experiments) are shown to enable supercontinuum generation in an isolated fundamental supermode, with the manifold of other PCF modes suppressed due to the strong evanescent fields coupling between the cores, providing a robust 5.4 W coherent supercontinuum output with a high spatial and spectral quality within the range of wavelengths from 500 to 1700 nm.
24 March 2011 in Journal of Materials Chemistry
To tailor clusters of active ions in glasses is laborious but critical for obtaining high efficient luminescence. Here, we present a facile method to tailor clusters of active ions by using one kind of porous host, the nanoporous silica glass. The white light-emitting glasses were prepared by sintering of nanoporous silica glasses impregnated with Ce3+, Tb3+, Mn2+ and Al3+ ions. The combination of blue, green and red emissions of Ce3+, Tb3+ and Mn2+ ions in the glasses under ultraviolet light excitation create white light emissions. The fluorescence of the glasses under long-wavelength ultraviolet excitation are dependent on energy transfer processes between the active ions; and the Al3+ plays a key role in adjusting of the energy transfer processes.
11 July 2018 in High Power Laser Science and Engineering
Ytterbium-doped fibers have become the optimum gain media of high-power fiber lasers thanks to a simple energy structure, which strongly reduces the excited state absorption, and a low quantum defect and a high optic–optic conversion efficiency, which means the low thermal load. In this paper, we take a review of the current state of the art in terms of $\text{Yb}^{3+}$ doped fibers for high-power fiber lasers, including the development of the fabrication techniques. The research work to overcome the challenges for $\text{Yb}^{3+}$ doped fibers, which affect the stability of output power and beam quality, will be demonstrated. Direction of further research is presented and the goal is to look for a fiber design, to boost single fiber output power, stabilize the laser power and support robust single-mode operation.
26 April 2017 in Optics Express
We have demonstrated a helical long-period grating (HLPG) manufactured from multicore fiber (MCF) combined with twist and CO2-laser heating technology. The MCF we used behaves as a kind of single mode fiber. The nineteen cores of MCF are distributed hexagonally which make the helical structure only exist in core area after heating and twisting. There are several strong couplings between the core and cladding modes at different wavelengths when the grating pitch was 900 µm. The extinction ratio of the main coupling reached 20 dB at 1550 nm. We have investigated the sensor characteristics of the HLPG. It is found that the grating presents clear sensitivity to refractive-index while exhibiting smaller cross-sensitivity to environmental temperature than conventional long-period gratings. The HLPG also shows great potential as a twist sensor, which has a sensitivity up to 0.198 nm/(rad/m) and can apply for measuring twist directions.
19 April 2018 in Applied Optics
A confined-doped fiber was fabricated by a modified chemical vapor deposition (MCVD) process based on refractive index matching technology. With theory and experiments, we compared the confined-doped fiber and normal-doped fiber. We found that the confined-doped fiber with a core of 35 μm and 0.07 numerical aperture could achieve single-mode output and improve the beam quality from 2.8 to 1.5 in the fiber laser. Meanwhile, it still possesses high laser efficiency and has good stability of beam quality with the increase in pump power. It suggests that the confined-doped fiber with a MCVD process may be the key material for a high-power fiber laser with excellent beam quality.
22 September 2010 in Optics Express
We report on a new kind of green-emitting high silica luminous glass, which is fabricated by sintering of Ce3+-Tb3+ co-doped porous glass. The spectra show that there are energy transfer between Ce3+ and Tb3+, and cross-relaxation between 5D3 and 5D4 energy level of Tb3+. The energy transfer process can be adjusted by addition of Ca2+ into the Ce3+-Tb3+ co-doped porous glass, and the transfer rate can be enhanced about four times than that of Ce3+-Tb3+ co-doped porous glass. The role of Ca2+ has been discussed, and the fluorescence decay curve reveals that the Ca2+ play an important role in energy transfer.