As ferroelectric Hf0.5Zr0.5O2(HZO) thickness scales below 10 nm, the switching characteristics are severely distorted typically showing an antiferroelectric-like behavior (pinched hysteresis) with reduced remanent polarization. Using Landau-Ginsburg-Devonshire (LGD) theory for the analysis of the experimental results, it is shown here that, in thin (5 nm) HZO, depolarization fields drive the system in a stable paraelectric phase coexisting with a metastable ferroelectric one, which explains the pinched hysteresis. This state of matter resembles a first order ferroelectric above the Curie temperature which is known to result in similar double-loop behavior. Here, based on the analysis of experimental data in the framework of LGD theory, it is reported that charge injection and trapping at pre-existing interface defects during field cycling (“wake-up”) screens the depolarization field stabilizing ferroelectricity. It is found in particular that a sufficiently large energy density of interface states is beneficial for the recovery of fully open ferroelectric loops.
The reliability of Hf0.5Zr0.5O2 (HZO) metal–ferroelectric–semiconductor capacitors grown by plasma-assisted atomic oxygen deposition on Ge substrates is investigated with an emphasis on the influence of crystallization annealing. The capacitors show very weak wake-up and imprint effects, allowing reliable operation in excess of 10 years, which is attributed partly to the clean, oxide-free Ge/HZO bottom interface. The weak temperature dependence and the observed asymmetries between polarization up and down states and between positive and negative coercive voltage shifts lead to the conclusion that imprint is controlled by carrier injection at the top electrode interface. The latter mechanism is associated with trapping at interfacial oxygen-vacancy defects. On the other hand, using ultrafast (millisecond) flash annealing improves the leakage current by at least an order of magnitude and the endurance by a factor of 3 compared to conventional rapid thermal annealing, which makes them suitable for low power nonvolatile memory applications where (ultra)thin HZO is an essential requirement.
Germanium Metal-Ferroelectric-Semiconductor (MFS) capacitors based on ferroelectric Hf1−xZrxO2 (HZO) with clean, oxide free Ge/HZO interfaces emerge as an interesting layer structure for the fabrication of ferroelectric field effect transistor (FeFET) non-volatile memory devices. It is shown that, at low temperature (<160 K), a semiconductor depletion forms in Ge near the interface, resulting in an increase in coercive voltage by about 2 V, accompanied by a distortion of the ferroelectric hysteresis with subloop asymmetric behavior, which becomes more severe at higher frequencies of measurement. At higher temperatures, the Ge surface near the ferroelectric is easily inverted due to the low energy gap of Ge, providing sufficient screening of the polarization charge by minority free carriers, in which case, nearly ideal, symmetric hysteresis curves are recovered. The depolarization field is experimentally extracted from the coercive voltage and the capacitance measurements, is found to be ∼ 2.2 MV/cm in the low temperature range, comparable to the coercive field, then rapidly decreases at higher temperatures, and effectively diminishes at room temperature. This makes Ge MFSs good candidates for FeFETs for low voltage non-volatile memory with improved reliability.
One monolayer semimetallic HfTe2 thin films are grown on three substrates with different electronic properties in order to study the substrate effect on the electronic structure of the HfTe2 epilayer. Angle resolved photoelectron spectroscopy measurements indicate that the band features are identical in all three cases, providing evidence that the HfTe2 epilayer does not interact with any of the substrates to form hybridized bands and any band feature originates from the HfTe2 material itself. However, a shift of HfTe2 energy bands is observed among the three cases, which is attributed to substrate electron doping. This paves the way for accessing the Dirac point of HfTe2 Dirac semimetal, which is located about ∼0.2 to 0.3 eV above the Fermi level in the case of suspended HfTe2 in a non-destructive way.