This study presents the strength development and durability of heat and non-heat-cured geopolymer mortars (GMs) produced using metakaolin (MK), ground granulated blast-furnace slag (GGBFS), silica fume (SF), ground calcined perlite (GCP), raw perlite (RP), potassium hydroxide (KOH), sodium metasilicate (Na2SiO3), standard sand, and tap water. An optimal combination of MK with various pozzolans and constant solid/liquid and alkaline activator ratios were determined. It was found that the GMs, including MK and GGBFS with a 1.45 solid/liquid ratio and 2.0 alkaline activator ratio, resulted in compressive strength at 88 MPa. Analysis of GMs was performed using scanning electron microscopy (SEM), EDX (Energy Scattered X-ray Spectrophotometer), and X-ray diffraction (XRD). According to the results obtained, mainly alumino-silicate-based formation, potassium from KOH solution, and calcium from GGBFS were determined. The SEM images showed that the grains with high silica content, approximately 6–7 µm in size, are quartz crystals and embedded in the gel structure. The heat-cured GMs were exposed to MgSO4, Na2SO4, and HCl solutions for the durability tests. The strength of the heat-cured GMs was higher than the non-heat-cured GMs, and the durability of the heat-cured GMs was found as sufficient. The use of pozzolans in GMs resulted in improvements in terms of strength and durability.
1 March 2013 in Construction and Building Materials
This study presents the strength development and characterisation of geopolymer mortars containing finely ground calcined perlite (GCP) as a precursor which is activated with sodium hydroxide (NaOH) solution. For this purpose, mortar specimens were produced with CEN standard sand, GCP, water and NaOH. The specimens subjected to heat curing after 24 h from casting and kept at an ambient temperature until the day of testing. The unit weight, ultrasound pulse velocity, flexural and compressive strengths of the mortar specimens were obtained after dry curing. The experimental results revealed that the mechanical properties of the mortars improved as the curing period and heat-curing temperatures increase, as well as increasing the concentration of NaOH. In addition, the characteristics of the mortars were determined by SEM/EDS and XRD analyses. According to the experimental results, the compressive strength of 37 MPa were obtained, and it is concluded that GCP can be used in geopolymer mortars owing to its abundance and appropriate chemical composition.