Li-ion batteries as a support for future transportation have the advantages of high storage capacity, a long life cycle, and the fact that they are less dangerous than current battery materials. Li-ion battery components, especially the cathode, are the intercalation places for lithium, which plays an important role in battery performance. This study aims to obtain the LiNixMnyCozO2 (NMC) cathode material using a simple flash coprecipitation method. As precipitation agents and pH regulators, oxalic acid and ammonia are widely available and inexpensive. The composition of the NMC mole ratio was varied, with values of 333, 424, 442, 523, 532, 622, and 811. As a comprehensive study of NMC, lithium transition-metal oxide (LMO, LCO, and LNO) is also provided. The crystal structure, functional groups, morphology, elemental composition and material behavior of the particles were all investigated during the heating process. The galvanostatic charge–discharge analysis was tested with cylindrical cells and using mesocarbon microbeads/graphite as the anode. Cells were tested at 2.7–4.25 V at 0.5 C. Based on the analysis results, NMC with a mole ratio of 622 showed the best characteristicd and electrochemical performance. After 100 cycles, the discharged capacity reaches 153.60 mAh/g with 70.9% capacity retention.
Zinc oxide (ZnO) is one of the most promising materials applied in Li-ion batteries. In this research, ZnO was synthesized by the thermal decomposition of zinc oxalate dihydrate. This precursor was obtained from the precipitation process of zinc sulfate with oxalic acid. In-depth studies were carried out on the effect of various heating temperatures of zinc oxalate dihydrate precursors on ZnO synthesis. The as-prepared materials were characterized by XRD, SEM, and FTIR. Based on the XRD analysis, the presence of the ZnO-wurtzite phase can be confirmed in samples heated at temperatures above 400 °C. Meanwhile, SEM-EDX results showed that the ZnO particles have a micron size. Cells with ZnO samples as anodes have low columbic efficiency. In contrast, cells with ZnO/Graphite composite anodes have a relatively large capacity compared to pure graphite anodes. Overall, based on the consideration of the characterization results and electrochemical performance, the optimal sintering temperature to obtain ZnO is 600 °C with a cell discharge capacity of ZnO anode and in the form of graphite composites is 356 mAh/g and 450 mAh/g, respectively. This suggests that ZnO can be used as an anode material and an additive component to improve commercial graphite anodes’ electrochemical performance.