Nanohybrid assemblies provide an effective platform for integrating the intrinsic properties of individual components into microscale fibers. In this study, a novel approach for creating mechanically and environmentally stable MXene fibers through the synergistic assembly of MXene and polyacrylonitrile (PAN), is introduced. Unlike fibers generated via a conventional stabilization process, which relies on air‐based stabilization to transform the PAN molecules into ring structures fundamental to carbon fibers, the hybrid fibers are annealed in an Ar atmosphere. This unique approach suggests MXene can serve as an oxygen provider that is essential for stabilizing PAN. As a result, significantly improved interfiber compactness is achieved and the oxidation stability of MXene is enhanced under atmospheric conditions. The resulting fibers exhibit exceptional stability, even after extended exposure to high humidity and elevated temperatures. This highlights the suitability of the thermally annealed MXene‐PAN (T‐MX‐PAN) fibers as robust electric heating elements. Notably, these fibers consistently generate heat over 1800 bending cycles. When integrated into fabrics, they demonstrate the capability to generate sufficient heat for melting ice and rapid evaporation. This study highlights the potential of T‐MX‐PAN fibers as next‐generation wearable heaters and offers valuable insights into advancing wearable technology in demanding environments.
The rheological properties of polycarbonate/acrylonitrile-butadiene-styrene (PC/ABS) blends with various blend ratios are investigated at different temperatures to determine the shear dependent chain motions in a heterogeneous blend system. At low frequency levels under 0.1 rad/s, the viscosity of the material with a blend ratio of 3:7 (PC:ABS) is higher than that of pure ABS polymer. As the temperature increases, the viscosities of ABS-rich blends increase rather than decrease, whereas PC-rich blends exhibit decrease in viscosity. Results from the time sweep measurements indicate that ordered structures of PC and the formation and breakdown of internal network structures of ABS polymer occur simultaneously in the blend systems. Newly designed sequence test results show that the internal structures formed between PC and ABS polymers are dominant at low shear conditions for the blend ratio of 3:7 and effects of structural change and the presence of polybutadiene (PBD) become dominant at high shear conditions for pure ABS. The results of yield stress and relaxation time for PC/ABS blends support this phenomenon. The specimen with a blend ratio of 3:7 exhibited the highest value of yield stress at high temperature among others, which implies that the internal structure become stronger at higher temperature. The heterogeneity of ABS-rich blends increases whereas that of PC-rich blends decreases as temperature increases.