CaCu3Ti[ ]YxO[ ] (0[ ]0.12) ceramics were fabricated with conventional solid-state reaction method. Phase structure and microstructure of prepared ceramics were characterized by X-ray diffraction (XRD) and scanning electron microscopy (SEM), respectively. The impedance and modulus tests both suggested the existence of two different relaxation behavior, which were attributed to bulk and grain boundary response. In addition, the conductivity and dielectric permittivity showed a step-like behavior under 405[ ]K. Meanwhile, frequency independence of dc conduction became dominant when above 405[ ]K. In CCTO ceramic, rare earth element Y[ ] ions as an acceptor were used to substitute Ti sites, decreasing the concentration of oxygen vacancy around grain-electrode and grain boundary. The reason to the reduction of dielectric behavior in low frequencies range was associated with the Y doping in CCTO ceramic.
In this work, (NaBi)0.5−x(LiSm)xBi2Nb2O9 (NBN-xLS, x = 0.00–0.06) ceramics were fabricated by co-doping of LiSm into Na0.5Bi2.5Nb2O9. The traditional solid-phase technique was employed for the entire synthesis process. The impact of LiSm doping on the crystal structure, dielectric, ferroelectric, and piezoelectric properties, as well as the underlying conduction mechanisms in the NBN-xLS ceramics, was analyzed systematically. The XRD patterns and the Rietveld refinement revealed that lattice distortion reduced with an increase in the LiSm doping amount. The decrease in lattice distortion significantly contributed to its improved ferroelectric and piezoelectric characteristics. The results showed that the NBN-xLS ceramics were primarily p-type materials due to their bulk-limited conduction, with oxygen holes and vacancies acting as the conducting species, and the appearance of weak ion conduction at high temperatures. The NBN-0.04LS ceramic, in particular, displayed the highest performance, with Pr, Tc, and d33 values of 9.05 μC/cm2, 777 °C, and 25.2 pC/N, respectively. Additionally, the ceramic displayed remarkable thermal stability, with its d33 retaining 95.0% of its original value after annealing at 760 °C. These results demonstrate that LiSm co-doped Na0.5Bi2.5Nb2O9 ceramics have potential for use in high-temperature sensors.
24 October 2023 in The Journal of Chemical Physics
Double-atom catalysts (DACs) for harmful nitrate (NO3−) electroreduction to valuable ammonia (eNO3RR) is attractive for both environmental remediation and energy transformation. However, the limited metal loading in most DACs largely hinders their applications in practical catalytic applications. Therefore, exploring ultrahigh-density (UHD) DACs with abundant active metal centers and excellent eNO3RR activity is highly desired under the site-distance effect. Herein, starting from the experimental M2N6 motif deposited on graphene, we firstly screened the low-density (LD) Mn2N6 and Fe2N6 DACs with high eNO3RR activity and then established an appropriate activity descriptor for the LD–DAC system. By utilizing this descriptor, the corresponding Mn2N6 and Fe2N6 UHD–DACs with dynamic, thermal, thermodynamic, and electrochemical stabilities, are identified to locate at the peak of activity volcano, exhibiting rather-low limiting potentials of −0.25 and −0.38 V, respectively. Further analysis in term of spin state and orbital interaction, confirms that the electronic state effect similar to that of LD–DACs enable the excellent eNO3RR activity to be maintained in the UHD–DACs. These findings highlight the promising application of Mn2N6 and Fe2N6 UHD–DACs in nitrate electroreduction for NH3 production and provide impetus for further experimental exploration of ultrahigh-density DACs based on their intrinsic electronic states.
The investigation of environmentally friendly, Pb-free ceramic dielectric materials with excellent energy storage capability represents a fundamental yet challenging research direction for the development of next-generation high-power capacitors. In this study, linear dielectric Ca0.7La0.2(Mg1/3Nb2/3)O3 was added into [0.65BaTiO3–0.35(Na0.5Bi0.5)TiO3] to form a solid solution. The introduction of Ca0.7La0.2(Mg1/3Nb2/3)O3 modified the crystal structure, enhanced insulation performance and breakdown strength, and reduced hysteresis loss. These improvements collectively contributed to higher energy storage density and efficiency (η). The ceramic pellet with the optimal 10 mol% Ca0.7La0.2(Mg1/3Nb2/3)O3 demonstrated a higher retrievable energy density (~3.40 J cm−3) and efficiency (~81%) at a breakdown strength of 340 kV cm−1 compared to BaTiO3-based ferroelectric ceramics. The sample also exhibited good stability across a temperature range of 30–90 °C and a frequency range of 0.5–300 Hz. Thus, the as-prepared ceramics sample exhibited significant potential for pulsed power device applications.