Buried reinforced concrete (RC) pipes in water, irrigation and sewer networks are aging, and their renewal must be prioritized without excavation, yet few non-destructive methods measure the stiffness of the pipe–soil system directly. The Internal Loading Method (ILM) loads the pipe wall from inside, and its response has so far been reduced to a single linear slope. This preliminary study examines whether a forced-origin quadratic representation, y = ax2 + bx, can describe load-dependent changes in slope that this linear stiffness cannot, using one RC pipe under four deterioration states and three burial conditions (above ground, 30 cm and a simulated 60 cm; 45 loading cycles). The sign of a gave the direction of curvature of the fitted response (negative in 40 cycles), but its statistical support, evaluated separately, was found in 28 cycles (significantly negative in 27 and significantly positive in one); the magnitude of a did not follow deterioration severity. The mean initial tangent stiffness decreased by 38–51% from the original to the maximum state and was higher at 60 cm than at ground level in all four states of this specimen, by 19% at maximum deterioration and 42–53% otherwise. In this dataset, was the most consistent descriptor examined, and burial must be considered when ILM stiffness is interpreted. The results require confirmation on further specimens.
Evaluating the structural integrity of buried pipelines is challenging because direct inspection is difficult and soil–structure interaction influences behavior. This study investigates the Internal Loading Method (ILM) as a quantitative diagnostic technique for reinforced concrete (RC) pipes under varying burial and deterioration conditions. An RC pipe (inner diameter: 250mm; wall thickness: 30mm) was tested using a manual Internal Loading Device (ILD) in a soil box at three burial depths — ground level, 30cm, and 60cm — and four deterioration states, from sound to severely damaged. Internal load was applied by the ILD while load–deformation responses and strains were recorded. Pipe–soil system stiffness was quantified from the elastic–range load–deformation response, and its variation with deterioration state and burial depth was evaluated. The results show that the slope of the load–deformation curve, representing pipe–soil system stiffness, decreases consistently as deterioration increases. At the same burial depth, the slope for a minimally deteriorated pipe was up to 13.5% lower than that of an intact pipe, with this reduction becoming more pronounced under deeper burial. Conversely, increasing burial depth generally enhanced system stiffness through soil confinement; however, this beneficial effect diminished progressively as structural damage accumulated, becoming negligible in the severely damaged state. Furthermore, ILM detected stiffness variations across all tested deterioration states and burial depths, and a diagnostic load–deformation chart was developed to relate in–situ stiffness to structural condition. These findings establish ILM as a practical, non–destructive tool for rehabilitation prioritization in RC pipeline management.