The article provides an overview of the methods used for processing of red mud to extract rare earth elements (REEs). Red mud is a toxic and highly alkaline waste. Several methods have been adopted and been practiced all over the world for the processing of red mud. Complex processing of red mud is cost-effective since red mud contains elements such as iron, aluminum, titanium, calcium, and rare earth metals. It has been observed that the acid leaching of red mud can almost completely recover the rare earth elements in the solution with various individual techniques and also a combination of them. Therefore, the choice of extraction method depends on the form in which the element occurs in the solution. However, relatively low concentrations of rare earth in the solution and significant amounts of impurities increase the cost of getting the final commercial products. To ensure the cost-effectiveness of the process involving rare earth’s extraction from red mud, it is necessary to increase their content by several times. This article presents the various studies that have been carried out in these aspects and the possibility of making this resource a sustainable one for REE extraction with a special focus on scandium replenishment.
This study focuses on optimizing the alkali roasting conditions for chromite beneficiation tailings with the goal of enhancing chromium oxide (Cr2O3) extraction. Within the experimental framework, the variables included roasting temperature, the amount of added Na2CO3, and reaction time. The results revealed that temperature is the most critical factor directly affecting the extraction efficiency. Increasing the amount of Na2CO3 contributed to an increase in Cr2O3 recovery, although excessive addition may not be economically justified. The optimal conditions—1000 °C, 120%–130% Na2CO3 (relative to tailings mass), and 120 min—enabled a Cr2O3 extraction rate of up to 98.6% through aqueous leaching. The phase transformation analysis confirmed the breakdown of the spinel structure and formation of water-soluble sodium chromate. Microanalysis observations and measurements validated the progressive destruction of chromite grains and sodium enrichment in the reaction zones. The remaining leaching residue consisted of inert Na2Mg2Si2O7 and MgO, suitable for further metal recovery. The proposed approach enables efficient detoxification of hazardous tailings and serves as a basis for integrated utilization of Cr-bearing industrial waste.
The global aluminium industry is ever-changing and primarily relies on bauxite as its traditional source. However, due to the finite reserves of processed bauxite, alternative sources need to be found. Nephelines have emerged as potential alumina sources. In addition to alumina, nepheline processing can yield marketable products such as soda, potash, cement, and rare metals.
30 April 2023 in Kompleksnoe Ispolzovanie Mineralnogo Syra = Complex Use of Mineral Resources
IUInstitute of Metallurgy and Beneficiation; Satbayev University
Institute of Metallurgy and Beneficiation; Satbayev University
AMA.I. Manapova
A.I. Manapova
+2
Due to limited reserves of bauxite, nepheline can be used in the industrial production of alumina in Kazakhstan. The most promising deposit is the nepheline syenites of the Kubasadyr deposit. Currently, there is no effective technology for processing nepheline ores. High energy intensity, capital intensity and significant emissions into the atmosphere are the main drawbacks of the conventional technology of nepheline ore processing by sintering method. Efficient hydrochemical processing of nepheline requires pre-enrichment with the separation of a part of silica. According to the existing technology of chemical enrichment in an alkaline solution at a temperature of 280⁰С, the silica extraction degree is no more than 36%. A pre-roasting at 500⁰C is used to increase the extraction rate of silica and this process permits an increase in the extraction rate to 65%. The paper presents the results of the chemical activation of nepheline syenites in a solution of sodium hydrogen carbonate. The optimum conditions of activation are determined. Activation at a temperature of 280 ⁰C resulted in a change in the phase composition of the feedstock and increases the degree of silica extraction up to 65,5%. The results obtained showed the possibility in principle of using hydrochemical enrichment technology for the resulting high-quality nepheline concentrate and replacing the energy-intensive roasting process.
When processing low-quality gibbsite–kaolinite bauxites, technologies that involve different methods of mechanical and chemical enrichment with the separation of a difficult-to-utilize fine kaolinite fraction for disposal are used. Before production, problems related to waste storage and disposal arise. To solve the problem of utilization, it is necessary to develop an effective technology for the selective processing of the kaolinite fraction. The efficiency of the technology will depend on the quality of pretreatment of raw materials prior to processing for Al2O3 extraction. Preliminary preparation of kaolinite fraction is associated with the maximum removal of excess silica during chemical enrichment by treatment with an alkaline solution. The presence of silica reduces the quality of final alumina products and requires a large consumption of reagents during the desiliconization of aluminate solutions. During the chemical enrichment of kaolinite fraction in alkaline solution, a serious problem of the co-dissolution of Al2O3 with silica arises. The solution to this problem can be the transformation of phase composition with the transformation of kaolin into a chemically resistant compound corundum, which will create conditions for the selective removal of silica. Kazakhstan’s alumina refinery, Pavlodar Aluminum Smelter, processes low-quality gibbsite–kaolinite bauxite from the Krasnogorsk deposit. To improve the quality of bauxite, preliminary gravity enrichment is carried out to separate the kaolinite fraction to a quantity greater than 50%. The purpose of this work was to study the possibility of the selective processing of the kaolinite fraction via various techniques, including preliminary thermal transformation, through sintering, chemical enrichment, autoclave leaching in a circulating aluminate solution, and low-temperature desiliconization, to obtain a solution for decomposition. As a result of this study, the possibility of obtaining a corundum phase after sintering at a temperature of 900–1000 °C was established, which made it possible to obtain 58.8% chemical enrichment through the extraction of SiO2 into solution. Further use of the enriched kaolinite fraction in autoclave leaching in a circulating aluminate solution with low-temperature desiliconization made it possible to obtain an aluminate solution with a caustic modulus of 1.65–1.7, which is suitable for decomposition.