Nguyen Thi Hoang Oanh

Prof. Dr. Nguyen Thi Hoang Oanh

Hanoi University of Science and Technology, Hanoi, Hà Nội, Vietnam
orcid

Research Focus & Metrics

Academic Career Length

20Years (2007-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 March 2007 in Materials Science and Engineering: A
Verified
Journal Article
Closed access
PCP.P. Choi
P.P. Choi
JKJ.S. Kim
J.S. Kim
NONguyen Thi Hoang Oanh
Nguyen Thi Hoang Oanh
DKD.H. Kwon
D.H. Kwon
YKY.S. Kwon
Y.S. Kwon
JKJ.C. Kim
J.C. Kim

29 March 2017 in Metals
Verified
Journal Article
Open access
PDF file
NONguyen Thi Hoang Oanh
Nguyen Thi Hoang Oanh
Nguyen Hoang VietNguyen Hoang Viet
Nguyen Hoang Viet
JKJi-Soon Kim
Ji-Soon Kim
AJAlberto Moreira Jorge Junior
Alberto Moreira Jorge Junior
This study focuses on the fabrication and microstructural investigation of Cu–TiH2–C and Cu–Ti–C nanocomposites with different volume fractions (10% and 20%) of TiC. Two mixtures of powders were ball milled for 10 h, consequently consolidated by spark plasma sintering (SPS) at 900 and 1000 °C producing bulk materials with relative densities of 95–97%. The evolution process of TiC formation during sintering process was studied by using X-ray diffraction (XRD), scanning electron microscopy (SEM), and high resolution transmission electron microscopy (HRTEM). XRD patterns of composites present only Cu and TiC phases, no residual Ti phase can be detected. TEM images of composites with (10 vol % TiC) sintered at 900 °C show TiC nanoparticles about 10–30 nm precipitated in copper matrix, most of Ti and C dissolved in the composite matrix. At the higher sintering temperature of 1000 °C, more TiC precipitates from Cu–TiH2–C than those of Cu–Ti–C composite, particle size ranges from 10 to 20 nm. The hardness of both nanocomposites also increased with increasing sintering temperature. The highest hardness values of Cu–TiH2–C and Cu–Ti–C nanocomposites sintered at 1000 °C are 314 and 306 HV, respectively.

21 January 2020 in Metals
Verified
Journal Article
Open access
PDF file
NONguyen Thi Hoang Oanh
Nguyen Thi Hoang Oanh
Nguyen Hoang VietNguyen Hoang Viet
Nguyen Hoang Viet
The initial as-cast microstructure of high-chromium white cast iron (2.08% C, 12.1% Cr), including austenitic dendrites in a matrix of a eutectic mixture of austenite and M7C3 carbides. Heat treatment of as-cast iron leads to a transformation of the matrix from austenite to martensite phase. The secondary M23C6 carbide precipitated from matrix improving the hardness of sample from 48 HRC to 62 HRC. JMatPro simulations of volume fraction phase for Fe-C-Cr-Mn alloy shows M7C3 and austenite phases are stable at austenitization temperature (1000 °C). Eutectic carbide of M7C3 is a stable phase in the alloy which is undissolved in the matrix during the heat treatment process. The HR-TEM images of heat-treated sample revealed that both eutectic M7C3 carbide and ultrafine secondary M23C6 carbide particles distributed on the martensite matrix.

30 November 2022 in Journal of Materials Research
Verified
Journal Article
Closed access
PDF file
Nguyen Hoang VietNguyen Hoang Viet
Nguyen Hoang Viet
NDNam Binh Do
Nam Binh Do
NONguyen Thi Hoang Oanh
Nguyen Thi Hoang Oanh
CNCao Son Nguyen
Cao Son Nguyen
VTVan Trung Trinh
Van Trung Trinh
AJAlberto Moreira Jorge Junior
Alberto Moreira Jorge Junior

3 April 2017 in Metals
Verified
Journal Article
Open access
PDF file
NONguyen Thi Hoang Oanh
Nguyen Thi Hoang Oanh
Nguyen Hoang VietNguyen Hoang Viet
Nguyen Hoang Viet
JKJi-Soon Kim
Ji-Soon Kim
Dina DudinaDina Dudina
Dina Dudina
In this work, TiC–Cu composites containing 20 and 30 vol % of nano-sized titanium carbide (TiC) particles were prepared by powder metallurgy using copper powders with micrometer-sized and nanometer-sized particles. Mixtures of TiC and Cu powders were ball milled for 10 h and spark plasma sintered at 800–900 °C under an applied pressure of 50 MPa. The relative density of the sintered composites was 95.0%–96.5%. The composites fractured in a ductile mode. The crystallite size of the copper matrix in the composites prepared using the nanometer-sized copper powder was smaller than that in composites prepared using the micrometer-sized copper powder, which was confirmed by transmission electron microscopy (TEM). The hardness of the composites increased as the sintering temperature was increased from 800 to 900 °C. When the TiC content increased from 20 to 30 vol %, the hardness of the composites obtained from the micrometer-sized copper powder and sintered at 900 °C increased from 284 to 315 HV, while in composites obtained from the nanometer-sized copper, the hardness decreased from 347 to 337 HV.

1 September 2007 in Materials Letters
Verified
Journal Article
Closed access
PCP.P. Choi
P.P. Choi
JKJ.S. Kim
J.S. Kim
NONguyen Thi Hoang Oanh
Nguyen Thi Hoang Oanh
YKY.S. Kwon
Y.S. Kwon