The purpose of this study was to assess the potential for biocomposite films to biodegrade in diverse climatic environments. Biocomposite films based on polyethylene and 30 wt.% of two lignocellulosic fillers (wood flour or flax straw) of different size fractions were prepared and studied. The developed composite films were characterized by satisfactory mechanical properties that allows the use of these materials for various applications. The biodegradability was evaluated in soil across three environments: laboratory conditions, an open field in Russia, and an open field in Costa Rica. All the samples lost weight and tensile strength during biodegradation tests, which was associated with the physicochemical degradation of both the natural filler and the polymer matrix. The spectral density of the band at 1463 cm−1 related to CH2-groups in polyethylene chains decreased in the process of soil burial, which is evidence of polymer chain breakage with formation of CH3 end groups. The degradation rate of most biocomposites after 20 months of the soil assays was greatest in Costa Rica (20.8–30.9%), followed by laboratory conditions (16.0–23.3%), and lowest in Russia (13.2–22.0%). The biocomposites with flax straw were more prone to biodegradation than those with wood flour, which can be explained by the chemical composition of fillers and the shape of filler particles. As the size fraction of filler particles increased, the biodegradation rate increased. Large particles had higher bioavailability than small spherical ones, encapsulated by a polymer. The prepared biocomposites have potential as an ecofriendly replacement for traditional polyolefins, especially in warmer climates.
Biocomposites based on low density polyethylene (LDPE) and birch wood flour (WF) were investigated. The mechanical properties and water absorption capacity were examined depending on the particle size of a filler in biocomposites. The aim of the paper is the investigation of composite properties depending on the filler particle size. The filler particle sizes were 0–80 µm, 80–140 µm, 140–200 µm, and 0–200 µm. The tensile strength of composite samples varied within the range 5.7–8.2 MPa. Elongation at break of composites varied within the range 5.1–7.5%. Highest mechanical properties were found in composites with the lowest filler fraction. Highest water absorption was observed in composition with a complex fraction of the filler. The influence of the filler particle size on composite properties was shown. It was found that an increase of the filler particle size decreases mechanical parameters and increases water absorption.
Lignosulfonate is a cheap material available in large quantities obtained as a byproduct of paper and cellulose. In this work, blends of polypropylene (PP) and sodium lignosulfonate (LGNa) were developed to evaluate the potential use of lignosulfonate as a lightweight, thermal insulation and flame retardant material. The blends were obtained by mixing in a torque rheometer and molded after compression. The blend proprieties were evaluated by physical, morphological, thermal, thermal conductivity, and flammability tests. The measured values were compared with theoretical models. The results indicated that a heterogeneous blend with a higher number of separated domains is formed when the LGNa content increases from 10 to 40 wt%. In addition, the density and thermal conductivity coefficient of the blends studied are not affected by the addition of LGNa. However, when the LGNa content in the blend exceeds 20 wt% the thermal stability and flame retardant proprieties are considerably reduced. The theoretical models based on the rule of mixtures showed a good agreement with the experimental values obtained from blend density, thermal conductivity, and thermal stability. In general, lignosulfonate tested in this work shows potential to be used as a reactive component in polymer blends.