Identifying novel cellulose fiber bio-composites has become a vital initiative in the exploration of sustainable materials due to increased global concern for the environment. This growing focus on eco-friendly materials has gathered significant attention in recent years. The current investigation deals with one such material, Helicteres isora reinforced Polylactic acid composites. Surface chemical treatment of fiber is one of the most effective methods to modify the hydrophilic fiber to increase its compatibility with the polymer matrix. Sodium hydroxide was used as a pre-treatment chemical to remove any impurities from the fiber surface. Pre-treated fibers were treated with Methacryl silane and Potassium permanganate solution to chemically modify the fiber surface. Density, void content and water absorption behavior of the composites were analyzed as per the standard procedure. Tensile and flexural tests were conducted to evaluate the mechanical strength, modulus, and flexibility of the unidirectional composites. Thermogravimetric and differential thermal analyses were performed to investigate the thermal stability, melting behavior and degradation profiles of prepared composites. A study of failure mechanisms and morphology of the fractured surface through photographs and SEM images revealed fiber splitting and delamination as the dominant reasons behind the failure of composites under tensile loading. Silane-treated Helicteres isora fiber-reinforced Polylactic acid composite exhibited lower water absorption and higher tensile strength than its counterparts. Untreated fiber composite showed maximum flexural strength among the tested composites. By collectively evaluating the results of the tests and properties of the composites, silane-treated fiber-reinforced Polylactic acid composites stands out as the most favorable choice.
The present study investigated the tensile behavior, failure mechanisms and deformation characteristics of glass fiber-reinforced polymer (GFRP) composites with symmetric [0°/90°/90°/0°] and asymmetric [0°/90°/0°/90°] stacking sequences across a temperature range of 30–150 °C. Tensile testing revealed superior mechanical performance in the symmetric lay-up, with higher tensile strength and failure strain sustained across elevated temperatures. Failure mode analysis revealed a transition from ductile failure to brittle failure with increasing temperature, which was more pronounced in the asymmetric lay-up, along with increased delamination and reduced fiber pull-out. Failure surface examination supported these findings, revealing better interfacial bonding and matrix integrity in the symmetric lay-up. Deformation analysis further confirmed a more homogeneous distribution of strain and longer failure time in symmetric laminates. Across all the metrics, including toughness, energy absorption, and strain uniformity, the symmetric configuration outperformed the asymmetric counterpart, underscoring the critical role of balanced stacking in enhancing the thermal durability. The observed temperature-induced degradation and its impact on mechanical and failure behavior emphasize the need for temperature-sensitive design strategies in GFRP-based structures.
Natural fiber-reinforced composites have gained significant attention due to their environmental benefits and desirable mechanical properties, including inherently beneficial vibration damping and acoustic characteristics. In this study, untreated, Alkali, Silane and Permanganate-treated Helicteres isora fiber-reinforced Polylactic acid composites were assessed to determine the effect of fiber treatment on the vibration and acoustic behaviour of the composites. Vibrational analysis was conducted to identify natural frequencies and damping ratios of the composites. The results demonstrated that alkali-treated fiber composite significantly enhanced the vibrational properties of the composites, with a 30% increase in damping ratio compared to untreated fiber composites. Acoustic transmission loss (TL) was measured to assess their suitability as soundproofing material using the impedance tube method. The results showed that silane-treated composites offered the highest TL in the frequency range 4000 to 6300 Hz, 35% more than untreated fiber composites, indicating their potential as an effective material in applications requiring soundproofing. In contrast, untreated fibers provided the lowest TL, affirming the impact of fiber modifications on acoustic performance. This study demonstrates that fiber modifications play a significant role in optimizing the vibrational and acoustic behaviour of natural fiber-reinforced bio-composites, making them a viable alternative for lightweight structural and noise-reducing applications.