Svetlana Petrova

Dr. Svetlana Petrova

Institute of Macromolecular Chemistry v.v.i., Academy of Sciences of the Czech Republic, Heyrovskeho nam. 2, CZ-162 00 Prague, Czechia

Research Focus & Metrics

Academic Career Length

18Years (2009-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
26 February 2018 in Nanoscale
Verified
Journal Article
Closed access
PDF file
Damir KlepacDamir Klepac
Damir Klepac
HKHana Kostková
Hana Kostková
SPSvetlana Petrova
Svetlana Petrova
Petr ChytilPetr Chytil
Petr Chytil
Tomas EtrychTomas Etrych
Tomas Etrych
Sergey FilippovSergey Filippov
Sergey Filippov
In this paper, we revised the current understanding of the protein corona that is created on the surface of nanoparticles in blood plasma after an intravenous injection. We have focused on nanoparticles that have a proven therapeutic outcome. These nanoparticles are based on two types of biocompatible amphiphilic copolymers based on N-(2-hydroxypropyl)methacrylamide (HPMA): a block copolymer, poly(ε-caprolactone) (PCL)-b-poly(HPMA), and a statistical HPMA copolymer bearing cholesterol moieties, which have been tested both in vitro and in vivo. We studied the interaction of nanoparticles with blood plasma and selected blood plasma proteins by electron paramagnetic resonance (EPR), isothermal titration calorimetry, dynamic light scattering, and cryo-transmission electron microscopy. The copolymers were labeled with TEMPO radicals at the end of hydrophobic PCL or along the hydrophilic HPMA chains to monitor changes in polymer chain dynamics caused by protein adsorption. By EPR and other methods, we were able to probe specific interactions between nanoparticles and blood proteins, specifically low- and high-density lipoproteins, immunoglobulin G, human serum albumin (HSA), and human plasma. It was found that individual proteins and plasma have very low binding affinity to nanoparticles. We observed no hard corona around HPMA-based nanoparticles; with the exception of HSA the proteins showed no detectable binding to the nanoparticles. Our study confirms that a classical “hard corona–soft corona” paradigm is not valid for all types of nanoparticles and each system has a unique protein corona that is determined by the nature of the NP material.

1 July 2015 in European Polymer Journal
Verified
Journal Article
Closed access
PČPeter Černoch
Peter Černoch
SPSvetlana Petrova
Svetlana Petrova
ZČZulfiya Černochová
Zulfiya Černochová
JKJoon-Sung Kim
Joon-Sung Kim
CSChristopher P. Simpson
Christopher P. Simpson
AAAlexandru Asandei
Alexandru Asandei

17 February 2014 in Polymer Chemistry
Verified
Journal Article
Closed access
PDF file
SPSvetlana Petrova
Svetlana Petrova
EJE. Jäger
E. Jäger
Rafał KonefałRafał Konefał
Rafał Konefał
AJA. Jäger
A. Jäger
CVC. G. Venturini
C. G. Venturini
PŠP. Štěpánek
P. Štěpánek
A new biocompatible and biodegradable diblock copolymer that contains a specific acid-labile degradable linkage (acyclic ketal group) between the hydrophobic poly(ε-caprolactone) (PCL) and the hydrophilic poly(ethylene oxide monomethyl ether) (MPEO) blocks is described herein. A multi-step synthetic method that combines carbodiimide chemistry, a “click” reaction and ring-opening polymerization (ROP) was employed to successfully produce a series of MPEO-b-PCL diblock copolymers (herein referred to as MPEO44-b-PCL17 and MPEO44-b-PCL44). 2-{[2-(2-Azidoethoxy)propan-2-yl]}ethan-1-ol was obtained as a linker between the two blocks through a three-step synthetic approach. Furthermore, a newly developed α-methoxy-ω-hydroxy-poly(ethylene oxide) that contains an acid-labile ketal linkage was designed as a macroinitiator via a “click” reaction for the sequential controlled ring-opening polymerization of ε-CL. The newly obtained compounds (precursors, macromer, macroinitiator and final diblock copolymers) were assessed by 1H NMR, 13C NMR and FT-IR spectroscopy and SEC analysis, which are described in this manuscript. Upon dissolution in a mild organic solvent, the MPEO44-b-PCL17 block copolymer self-assembled in water–PBS into regular, spherical, stable nanoparticles (NPs). Furthermore, the presence of the acid-labile ketal linker enabled the disassembly of these nanoparticles in a buffer that simulated acidic cytosolic or endosomal conditions in tumour cells as evaluated by dynamic light scattering (DLS), nanoparticle tracking analysis (NTA) and transmission electron microscopy (TEM) images. This disassembly led to hydrolysis profiles that resulted in neutral degradation products.

2 June 2016 in RSC Advances
Verified
Journal Article
Closed access
PDF file
PČPeter Černoch
Peter Černoch
ZČZulfiya Černochová
Zulfiya Černochová
SPSvetlana Petrova
Svetlana Petrova
DKDana Kaňková
Dana Kaňková
JKJoon-Sung Kim
Joon-Sung Kim
AAAlexandru Asandei
Alexandru Asandei
A visible light, Mn2(CO)2-photomediated process was used to enable the iodine degenerative transfer controlled radical polymerization of vinylidene fluoride (VDF) initiated from I–(CF2)6–I, and the successive quantitative activation of the ∼CH2–CF2–I and ∼CF2–CH2–I chain ends of I–PVDF–I, to produce a series of PNpSS-b-PVDF-b-PNpSS triblock copolymers (NpSS/VDF/NpSS = 4/60/4, 15/60/15, 34/60/34) with neopentyl styrene sulfonate (NpSS), which upon NaN3 deprotection, afforded the corresponding PNaSS-b-PVDF-b-PNaSS. All blocks, as well as PVDF, PNpSS and PNaSS formed water stable dispersion/solutions following either nanoprecipitation from acetone (PVDF, PNpSS, and PNpSS-b-PVDF-b-PNpSS) or direct dissolution in water (PNaSS, PNaSS-b-PVDF-b-PNaSS). Remarkably, all PNaSS-b-PVDF-b-PNaSS triblocks also provided indefinitely stable systems even under the high ionic strength conditions of phosphate buffered saline (PBS) solutions, corresponding to cell-isotonic, pH = 7.4 conditions. These trends were found to be consistent with the block composition dependence of the apparent hydrodynamic radius (Rh), conductivity, and zeta potential (ζ), where Rh increases upon deprotection from about 35–25 nm to about 168–136 nm in water, and decreases to 133–86 nm in PBS solutions, ζ decreases from ∼−40 mV to ∼−70 mV in water and increases to ∼−18 mV in PBS, and where the conductivity is negligible for PNpSS-b-PVDF-b-PNpSS but then increases linearly to ∼0.2 mS cm−1 for PNaSS-b-PVDF-b-PNaSS in water to reach ∼17 mS cm−1 in PBS. Finally, the blocks were evaluated as promising 19F-MRI contrast agents.

31 December 2009 in European Polymer Journal
Verified
Journal Article
Closed access
SPSvetlana Petrova
Svetlana Petrova
RRRaphaël Riva
Raphaël Riva
Christine JeromeChristine Jerome
Christine Jerome
Philippe LecomtePhilippe Lecomte
Philippe Lecomte
RMRosa Mateva
Rosa Mateva

27 July 2016 in Macromolecules
Verified
Journal Article
Closed access
SPSvetlana Petrova
Svetlana Petrova
Damir KlepacDamir Klepac
Damir Klepac
Rafał KonefałRafał Konefał
Rafał Konefał
SKSami Kereïche
Sami Kereïche
LKLubomír Kováčik
Lubomír Kováčik
Sergey FilippovSergey Filippov
Sergey Filippov