Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology
Mr. Xingheng Yan
Science and Technology on Advanced Ceramic Fibers and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology
The MAX phase Ti3SiC2 has broad application prospects in the field of rail transit, nuclear protective materials and electrode materials due to its excellent electrical conductivity, self-lubricating properties and wear resistance. Cu-Ti3SiC2 co-continuous composites have superior performance due to the continuous distribution of 3D network structures. In this paper, the Cu/Ti3SiC2(TiC/SiC) co-continuous composites are formed via vacuum infiltration process from Cu and Ti3SiC2 porous ceramics. The co-continuous composites have significantly improved the flexural strength and conductivity of Ti3SiC2 due to the addition of Cu, with the conductivity up to 5.73×105 S/m, twice as high as the Ti3SiC2 porous ceramics and five times higher than graphite. The reaction between ingredients leads to an increase in the friction coefficient, while the hard reaction products (TiCx, SiC) lower the overall wear rate (1×10−3 mm3/(N•m)). Excellent electrical conductivity and wear resistance make co-continuous composites more advantageous in areas such as rail transit.
B4C–TiB2 composite ceramics with ultra-high fracture toughness were successfully prepared via spark plasma sintering (SPS) at 1900 °C using B4C and Ti3SiC2 as raw materials. The results showed that compared with pure B4C ceramics sintered by SPS, the hardness of B4C–TiB2 composite ceramics was decreased, but the flexural strength and fracture toughness were significantly improved; the fracture toughness especially was greatly improved. When the content of Ti3SiC2 was 30 vol.%, the B4C–TiB2 composite ceramic had the best comprehensive mechanical properties: hardness, bending strength and fracture toughness were 27.28 GPa, 405.11 MPa and 18.94 MPa·m1/2, respectively. The fracture mode of the B4C–TiB2 composite ceramics was a mixture of transgranular fracture and intergranular fracture. Two main reasons for the ultra-high fracture toughness were the existence of lamellar graphite at the grain boundary, and the formation of a three-dimensional interpenetrating network covering the whole composite.