• The Proposed multi-microjet impact model suitable for high hydrostatic pressures. • Cavitation erosion experiments can be conducted in an ultrasonic cavitation system composed of a spherical cavity focused transducer with high acoustic energy in a sub-wavelength focal region. • Quantitative analysis of cavitation pit morphology can be achieved through the proposed microjet impact model. • A microjet velocity inversion model was proposed to quantitative evaluate the cavitation erosion intensity.
Cavitation erosion is a general phenomenon in the fields of aviation, navigation, hydraulic machinery, and so on, causing great damage to fluid machinery. With the vast requirements in deep ocean applications, it is urgent to study the mechanism of cavitation erosion and the cavitation erosion resistance of different materials under high hydrostatic pressure to predict and avoid the effect of cavitation erosion. In this work, the spatially confined cavitation bubble cloud associated with Gaussian-like intensity distribution sonoluminescence (SL) was produced by a spherically focused ultrasound transducer with two opening ends near metallic plates under different hydrostatic pressures (0.1, 3, 6, and 10 MPa). The cavitation erosion effects on copper, 17-4PH stainless steel and tungsten plates were studied. Through coupling analysis towards the SL intensity distribution, the macro/micro morphology of cavitation erosion, and the physical parameters of different metallic materials (hardness, yield strength, and melting point), it is found that with increasing hydrostatic pressure, the erosion effect is intensified, the depth of cavitation pits increases, the phenomenon of melting can be observed on materials with relatively low melting points, and the cavitation erosion experienced an evolution process from high-temperature creep to fracture. This work has also established a method for the evaluation of materials' cavitation erosion resistance with measurable SL intensity distribution, which is promising to promote the designing and selection of anti-cavitation materials in deep-sea applications.
The near-solid wall multi-bubble cavitation is an extremely complex phenomenon, and cavitation has strong erosiveness. The melting point (about 3410 °C) of tungsten is highest among all pure metals, and its hardness is also very high (its yield strength is greater than 1 GPa). What would happen to pure tungsten wire under extreme conditions caused by collapsing cavitation bubbles at high hydrostatic pressure? In this paper, we have studied the fracture process of pure tungsten wire with diameter of 0.2 mm mounted at the focus of a standing acoustic wave produced by a spherical cavity transducer with two open ends placed in a near spherical pressure container, and also studied the macro and micro morphological characteristics of the fracture and the surface damage at different fracture stages of tungsten wire under various hydrostatic pressures and driving electric powers. The results have shown that the fracture time of tungsten wire is inversely proportional to avitation intensity with hydrostatic pressure and driving electric power, the higher the acoustic pressure caused by higher electric power, the shorter the fracture time. The possible fracture mechanisms of tungsten wire in this situation we found mainly contributed to asymmetrically bubbles collapse near the surface of tungsten wire, leading to tearing the surface apart; consequently cracks along the radial and axial directions of a tungsten wire extend simultaneously, classified as trans-granular fracture and inter-granular fracture, respectively. With the increase of cavitation intensity, the cracks tend to extend more radially and the axial crack propagation path becomes shorter, that is, mainly for trans-granular fracture; with the decrease of cavitation intensity, intergranular fracture becomes more obvious. When the hydrostatic pressure was 10 MPa and the driving electric power was 2 kW, the fibers became softener due to the fracture of the tungsten wire. The fracture caused by acoustic cavitation was different from conventional mechanical fracture, such as tensile, shear, fatigue fracture, on macro and micro morphology.