The magnetic properties of ThMn12-type Fe-rich compounds were investigated by producing Sm(Fe0.8Co0.2)10Si2 ribbons. The produced ribbons, with different conditions by varying the melt-spinning conditions, were characterized to investigate physical and magnetic properties. Weight fraction of ThMn12-type phase decreased from 94.5 to 57.1 wt. % as the melt-spinning wheel speed increased from 6.5 to 39 m/s, and corresponding magnetizations and coercivities were substantially varied; the coercivity increased up to 0.175 T from 0.058 T by increasing the wheel speed from 6.5 to 26 m/s, and their magnetization also increased from 89.81 Am2/kg to 105.58 Am2/kg, even though the content of ThMn12-type phase decreased. Morphologies of the ribbons were also observed to verify the melt-spinning effects on the surface conditions and grain sizes. It was found that the particle and grain sizes in the ribbons became smaller and striped patterns appeared as the wheel speed increased. The grain size decreased from about 1 μm to 250 nm by increasing the wheel speed from 6.5 to 39 m/s.
9 April 2024 in Journal of Materials Research and Technology
Anisotropic bulk magnets of ThMn12-type SmFe10V2 with a high coercivity (Hc) were successfully fabricated. Powders with varying particle sizes were prepared using the ball milling process, where the particle size was controlled with milling time. A decrease in Hc occurred in the heat-treated bulk pressed from large-sized powders, while heavy oxidation excessively occurred in small powders, leading to the decomposition of the SmFe10V2 (1–12) phase. The highest Hc of 8.9 kOe was achieved with powders ball-milled for 5 h due to the formation of the grain boundary phase. To improve the maximum energy product ((BH)max), which is only 2.15 MGOe in the isotropic bulk, anisotropic bulks were prepared using the same powders. The easy alignment direction, confirmed by XRD and EBSD measurements, was . Significant enhancements were observed, with saturation magnetization (Ms) increasing from 59 to 79 emu/g and a remanence ratio (Mr/Ms) of 83.7%. (BH)max reaching 7.85 MGOe. For further improvement of magnetic properties, controlling oxidation is essential to form a uniform grain boundary phase and achieve perfect alignment with small grain size.
We explored the potential for an aging treatment to achieve high coercivity, of 0.859 MA/m, in a SmFe10V2 alloy with a ThMn12-type structure. Bulk magnets were fabricated by sintering ball-milled powders, followed by aging treatment. XRD and SEM analyses revealed that aging treatment promotes the formation of a Sm-rich grain boundary phase with nano-scale thickness. The high Sm content (~60–80 at.%) and low Fe content (~20–30 at.%) in the grain boundary phase led to non-ferromagnetism, enhancing the coercivity by isolating the 1–12 grains and weakening the dipolar interaction between the grains. The aging temperature and duration were optimized to maximize the Sm-rich phase and minimize the soft magnetic SmFe2 phase. This study provides a new fabrication method for ThMn12-type magnets and investigates the relationship between microstructure and coercivity, offering valuable insights for the future design and development of high-performance SmFe12-based magnets.