The aim of this paper is to determine the feasibility of submerged friction stir welding of 6061-T6 aluminium alloy on different water heads through macrostructuralanalysis.In this work, aluminium 6061-T6 alloy was friction stir welded under normal and submerged conditions at different rotational speeds of 400 rpm, 800 rpm, 1200 rpm, 1600 rpm. The water head was varied from 10 to 30 mm in the case of thesubmerged friction stir welding process. In both normal and submerged friction stir welding processes, a welding speed of 45 mm/min, a normal load of 30 kN, tool tilt angle of 2˚, depth of tool penetration and tool geometry were kept constant. Torque is measured during the welding process, and power (kW) is calculated after the welding process. The macrostructural analysis was carried out for locating defect formation and identifying the feasible working range of process parameters of the welded aluminium 6061-T6 alloy. The mechanical properties such as ultimate tensile strength and microhardness of submerged friction stir welded of 6061 aluminium alloys were investigated.Scanning Electron Microscope (SEM) metallography was used for comparing the microstructure of the parent material, friction stir welded and submerged stir welded samples.
20 July 2020 in Advances in Materials and Processing Technologies
Friction Stir Welding (FSW) uses friction and mechanical plastic deformation to heat and soften any weld material, allowing mechanical deformation comparable to extrusion and forging for enabling the formation of a highly strengthened joint. This paper reports the use of response surface methodology-based grey methods for the optimisation of the Submerged Friction Stir Welding (SFSW) process parameters, as joining the 6061-T6 aluminium alloy. The process parameters selected were the rotational speed (rpm), welding speed (mm/min) and water head (mm). Experiments were carried out on aluminium alloy using a servo controller FSW machine. The mechanical properties (average hardness and % of elongation) of submerged friction stir welded joints of the 6061-T6 aluminium alloy were investigated. The optimal welding process parameters for maximising the Avg.hardness and % of elongation were identified using the Grey Relation Analysis (GRA). Quadratic equation was developed for predicting the grey relational grade with good accuracy and fitted with adequate errors. The analysis of variance (ANOVA) was for testing to test the significance of the equation. The microstructural characteristics of the base metal and welded zone, as well as grain structure, were studied using scanning electron microscopy.
23 March 2021 in Journal of Materials Engineering and Performance
In this work, Inconel 625 alloy was used to manufacture walls using the Wire Arc Additive Manufacturing (WAAM) technology, which is based on Gas Tungsten Arc Welding (GTAW). The wall was fabricated using a circular weave and stringer bead pattern. Microstructural analysis and tensile characteristics were evaluated for both walls. Using scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and elemental mapping, the fracture zones of the tensile specimens were examined. The microstructure is mostly made up of equiaxed dendrites, with the rare presence of continuous and discontinuous cellular dendrites along the cross-section. In tensile tests, circular weaved walls performed better than stringer bead walls. The circular weave specimen had an ultimate tensile strength (UTS) of 762 MPa in the horizontal and 722 MPa in the vertical orientations. Also, the Inconel 625 wall showed anisotropic behavior (5.3%) during tensile testing. The fracture morphology analysis revealed that all the specimens were fractured as a result of large plastic deformation, corresponding to ductile failure. Based on the EDS results, the fracture zone mainly consists of Ni and Cr with a small percentage of Nb and Mo. The absence of laves phases makes the fracture mode ductile. The elemental mapping shows uniform dispersion of Ni and Cr within the fracture region, further supporting the ductile failure mode.