The LaFe1−xZrxO3 (x = 0.01, 0.05) ceramics were prepared by sol-gel and annealing method and studied by XRD, Raman scattering analysis, SEM, and impedance spectroscopy method. The crystal structure and phonon characteristics analysis revealed that the crystal structure tends to preserve its ideal orthorhombic structure, following the increase in driving force of the Fe/ZrO6 octahedral tilting. The frequency-dependent dielectric parameters at each temperature decreased with increasing Zr content. The temperature dependence dielectric relaxation and dc conduction mechanism satisfied the Arrhenius law and increased with increasing Zr content. The activation energy ranged from 0.30 to 0.50 eV and was similar in the relaxation and conduction mechanisms, indicating that both transport mechanisms were based on a similar mechanism.
24 September 2019 in Journal of Materials Science: Materials in Electronics
In this study, the effect of heat treatment on the structural, magnetic and electrical properties of La2FeMnO6 prepared via the sol–gel and sintering method were investigated. The heat-treatment conditions, i.e., the calcination temperature (1023 K and 1173 K), sintering temperature and time (1273 K for 1 and 3 h) were carried out. X-ray diffraction (XRD) revealed orthorhombic pnma (62) symmetry without any impurity phase for all samples. X-ray photoelectron spectroscopy confirmed the presence of Fe2+–Fe3+–Fe4+ and Mn3+–Mn4+ mixed states, and lanthanum and oxygen vacancies resulting in various magnetic exchange interactions. Furthermore, the magnetisation hysteresis showed enhanced hysteresis loops accompanied by an increase in magnetisation parameters with calcination temperature. The Raman phonon parameters induced a redshift in the phonon modes, alongside an increase in the intensity and compression of the linewidth, reflecting a decrease in lattice distortion, which was confirmed by XRD. The temperature-dependent conductivity showed that the conduction mechanism is dominated by p-type polaron hopping, and the lowest activation energy was approximately 0.237 ± 0.003 eV for the minimum heat-treatment conditions. These results show that varying heat-treatment conditions can significantly affect the structural, magnetic and electrical properties of the La2FeMnO6 system.
Magnetic properties and exchange couplings of nanocomposite magnets prepared by mechanical milling have been investigated at low temperatures. With decreasing temperature, due to Y substitution for Nd, an extension of the exchange coupling length in nanocomposite magnets occurs in a wider temperature range. This can be attributed a decreasing anisotropy of the hard-magnetic phase so that more soft-magnetic grains participate the exchange coupling. Close to 135 K, due to the spin reorientation, the hard magnetic phase is not more uniaxail, which leads to a drastic decrease of the magnetic properties of the -based nanocomposite magnets.