Decreasing the weight of heavy-duty vehicles is an ongoing concern. However, the need to deal with high temperatures in components such as manifolds imposes, by itself, some restrictions regarding material selection, being further limited when other required properties (e.g., functional, manufacturing or cost requirements) are taken into account. Cast austenitic stainless steels may represent a good choice in this context but the existence of concentrated chromium carbides can generate undesirable results. A good combination of heat treatments can be applied to cast heat-resistant austenitic stainless steels, in an effort to achieve the dispersion of fine carbides, consequently improving their microstructure, mechanical properties and creep resistance. In this work, an austenitic stainless steel usually used in high temperature applications was characterized and subjected to solution annealing and aging heat treatments. The material analyzed was the austenitic cast stainless steel HK30 and the goals of the work were to evaluate the effects of solution annealing heat treatments on the dissolution of grain boundary chromium carbides and the effects of aging treatments on creep resistance. The results show that the elimination of grain boundary chromium carbides is possible by applying a solution annealing heat treatment. Additionally, the precipitation of fine dispersed carbides is obtained after the aging treatment with an increase of hardness and, consequently, an expected improvement of creep resistance. Thus, the novelty presented by this work consists of selecting the best heat treatment combination in order to promote dispersion of carbides, thus avoiding further crack nucleation phenomena when parts are cyclically subjected to load and unload; this work also found the most adequate mechanical properties and achieved corrosion resistance regarding the application in heavy-duty vehicle components subjected to mechanical and thermal fatigue. By discovering methods of improving the properties of cast materials, large savings can be made both in terms of production costs as well as in the overall weight of the components.
2 July 2019 in Metallurgical and Materials Transactions A
The influence of cooling rate on the formation of iron-rich intermetallic phases during solidification of unmodified and strontium-modified Al-7Si-0.3Mg alloys has been investigated. The effect of strontium on the intermetallic phases was evaluated in unquenched and quenched samples. Samples were quenched before the start of the Al-Si eutectic reaction, along the Al-Si eutectic reaction and just after the end of solidification. The results show that the addition of strontium increased the size of both β-Al5FeSi and π-Al8FeMg3Si6 at low cooling rates. For unmodified and strontium-modified alloys, an increase of cooling rate resulted in a decrease in size of the intermetallic phases, particularly in the strontium modified alloy. In the strontium modified alloy quenched before the start of the Al-Si eutectic reaction, π-Al8FeMg3Si6 appeared as thin platelets at the eutectic cell boundaries. Chinese script-like π-Al8FeMg3Si6 and platelet-like β-Al5FeSi intermetallic phases were observed uniformly distributed in the eutectic regions in the unmodified alloy quenched before the start of the eutectic reaction. Strontium modified semi-solid Al-7Si-0.3Mg castings were produced and the type of intermetallic phase, morphology, size, area fraction and distribution were similar to that observed in the strontium modified alloy quenched before the start of the Al-Si eutectic reaction.
Magnesium and silicon concentrations in the interior of primary α-Al of Al-7Si-Mg alloys were studied at temperatures in the liquid-solid range and just after solidification was completed. Analysis of the results showed that the magnesium concentration in the interior of primary α-Al is very low in the temperatures range from the liquidus to the start of the Al-Si eutectic reaction. Formation of silicon-rich phases during eutectic reactions, such as eutectic silicon and β-Al5FeSi, phases trigger a significant increase in the magnesium concentration in the interior of primary α-Al, when sufficient time is allowed for solid-state diffusion to occur. When fast cooling rates are applied during the Al-Si eutectic reaction, most of the magnesium is retained in π-Al8FeMg3Si6 and Mg2Si phases formed during solidification. Semi-solid Al-7Si-Mg castings were produced with varying magnesium contents, and the mechanical properties were evaluated in the as-cast, T5 and T6 conditions. It was found that the 0.2% offset yield strength of the semi-solid Al-7Si-Mg castings in the T5 and T6 conditions increases linearly with the square root of the magnesium concentration in the interior of the α-Al globules formed during the slurry preparation process.
9 July 2018 in Metallurgical and Materials Transactions A
This study aims to evaluate the effect of grain refinement on slurry formation and surface segregation in semi-solid castings produced by the Rheometal™ process. The effect of two grain refiners, Al-8B and Al-5Ti-1B, on the slurry α-Al grain size, shape factor and solid fraction was evaluated. The results suggest that the addition of a grain refiner can affect the solid fraction obtained in the RheometalTM process and, consequently, reduce the solute content near the casting surface. Grain refiner addition resulted in a larger fraction of α-Al grains ≤ 60 µm for the refined alloys compared with the unrefined alloy. Additionally, the growth of α-Al slurry globules was greater for the unrefined alloy compared with the refined alloy during solidification in the die-cavity. A more homogeneous and finer microstructure was observed near the surface in the grain-refined castings compared with the unrefined castings. Evidence of significant liquid penetration was identified in some α-Al globules, indicating that disintegration of α-Al globules may occur during the Rheometal™ casting process.
30 September 2021 in Metallurgical and Materials Transactions A
Primary type polyhedral silicon crystals were observed in the vicinity of oxides located at or near the surface of strontium modified semi-solid Al–7Si–Mg castings. The coarse silicon polyhedrons were observed mainly on the outer side of oxides surrounding the macrosegregation regions. The silicon crystals most likely nucleated on AlP-particles located near the oxides. These AlP particles may nucleate on the wetted surface of oxides, or form at different locations in the interdendritic regions.
Four-point bending fatigue tests were performed on semi-solid Al–7Si–Mg castings with varying magnesium contents and heat treatment conditions. Additionally, the effect of anodising on the fatigue resistance of semi-solid Al–7Si–Mg castings was evaluated. Fracture surface and microstructure analysis showed that fatigue crack initiation occurred mainly at the periphery of regions of positive macrosegregation at the casting surface, resulting most likely from exudation. The microstructure of these macrosegregation regions was mostly eutectic and was frequently found surrounded by a layer of oxides. This layer of oxides promoted weak bonding between the macrosegregation region and the surrounding material and acted as a crack initiation site. In this study, primary α-Al globule agglomerates at the casting surface and surrounded by a layer of oxides also promoted fatigue crack initiation. Fatigue resistance of semi-solid Al–7Si–Mg castings in the T5 and T6 conditions increased with the increase in the magnesium content of the alloy from 0.3 to 0.45 wt.% due to the higher precipitation hardening response. However, the increase in the magnesium content from 0.45 to 0.6 wt.% resulted in a slight decrease in the fatigue resistance. The oxide layer formed during anodising had no significant effect on the fatigue resistance of the semi-solid Al–7Si–Mg castings in this study due to the dominant effect of the macrosegregation regions on fatigue crack initiation.