This study employed annealing heat treatment ranging from 900 to 1300 °C to systematically investigate the effects of annealing temperature on the microstructure and hydrogen storage performance of the equimolar TiZrCrMnFeNi high-entropy alloy. The research indicates that the TiZrCrMnFeNi high-entropy alloy is composed of the C14 Laves phase and a small amount of cubic phase. Compared to the as-cast alloy, the alloy annealed at high temperature (1000~1200 °C) exhibited increased microstructure homogeneity, a higher content of the C14 Laves phase, and a significant enhancement in hydrogen storage capacity. The annealing heat treatment led to changes in the unit cell volume of the C14 Laves phase, with an inverse relationship between unit cell volume and hydrogen absorption and desorption plateau pressures. An increase in unit cell volume resulted in a lower desorption plateau pressure, making the desorption reaction more difficult and consequently increasing the enthalpy change for desorption. This study not only reveals the intrinsic relationship between annealing temperature and the hydrogen storage performance of high-entropy alloys, but also provides significant experimental evidence and theoretical guidance for the design and development of high-entropy alloy materials with excellent hydrogen storage characteristics.
18 January 2022 in Transactions of the Indian Institute of Metals
Hydrogen absorption kinetics in metal hydride beds is constrained by coupled heat and mass transfer, which often leads to a slow refueling response and reduced storage system efficiency. In this work, hybrid molding by mixing silicone gel with various thermally conductive additives was used to prepare TiMn-based metal hydride beds with tailored porosity and thermal conductivity. Three experimental groups were prepared: 5 wt.% silicone gel and 5 wt.% single-walled carbon nanotubes (Group A), 5 wt.% silicone gel only (Group B), and 5 wt.% silicone gel and 5 wt.% silicone sheets (Group C). Hydrogen absorption kinetics at 30 °C and 50 bar were measured experimentally and simulated using a coupled heat-mass transfer model in COMSOL Multiphysics. The physical property results showed that Group A exhibited approximately threefold higher porosity (0.527) compared with the other two groups, while its thermal conductivity (2.476 W·m−1·K−1) was the lowest among them (3.189 W·m−1·K−1 for Group B and 3.246 W·m−1·K−1 for Group C). These property differences led to distinct hydrogen absorption rate-limiting behaviors. Group A dominated in the diffusion-controlled stage (hydrogen uptake between 0.5 and 1.15 wt.%) due to enhanced hydrogen transport through its macroporous network, while Group C exhibited faster kinetics in the later stage (above 1.15 wt.%), where thermal conductivity governed the absorption driving force. Numerical simulations reproduced the experimental kinetic curves and confirmed the transition of rate-limiting mechanisms. This work reveals that the rate-limiting factors of hydrogen absorption in hybrid molding hydride beds vary across different stages, and that independent optimization of porosity and thermal conductivity is required to achieve rapid kinetics across the entire absorption process.
20 July 2024 in Transactions of the Indian Institute of Metals