The prospects of processing blast furnace and steelmaking sludge using the Waelz process in a laboratory rotary kiln, is shown. The influence of different processing temperatures, furnace atmosphere and the type of reducing agents on the level of zinc reduction from sludges was analyzed. In general, the blast furnace sludge contains a high portion of iron (approx. 48 wt.%) and can be reused as a charge after satisfactory zinc reduction. It was found that N- atmosphere and a high content of the graphite or coke oven reducing agent in combination with high temperature can reduce the content of Zn in the sludge to 0.08 wt.% at 1200 °C for a mixture of steelmaking and blast furnace sludge. A significant reduction in the Zn content to 0.66 wt.% occurs at 1100 °C. The content and type of reducing agent plays an important role; graphite has shown a better reducing ability compared to coke oven dust. When nitrogen is used, zinc is reduced even without an additional reducing agent, since the carbon contained in the sludge is made use of for the reduction. In an air atmosphere, without the use of a reducing agent, there was no reduction in the Zn content.
The aim of this work is to compare the technological and material properties of CMnCr steels without bismuth, with 0.08 wt. % Bi and 0.12 wt. % Bi. Experimental heats showed that the most advantageous alloying of Bi into the heat was in the ladle, with an efficiency of about 20%. The optimal temperature range for forming steel was found to be 1160–1050 °C. With increasing Bi content, the formability of steels and plastic properties decreased, while the yield stress and tensile strength increased. Manganese sulfides, aluminum oxides, or oxysulfides, which were segregated both individually and in clusters, were found in the matrix of all tested steels. In steels with Bi, the Bi particles segregate the separately in the form of globules, either as envelopes of elongated MnS or Al2O3 particles segregated in rows. Sulfur dot-shaped segregations in the steel with 0.12 wt. % of Bi and the steel without Bi were essentially uniform over the whole area. For the steel with 0.08 wt. % of Bi, both dot-like and ray-ordered sulfur segregations were observed. The microstructure of all tested steels was ferritic–pearlitic with islands of bainite. Towards the center of the forged bars, variable shape and size of bainite blocks were observed. Machinability tests evaluated by the extend of tool wear showed that the most advantageous was CMnCr steel alloyed with 0.08 wt. % Bi.
The paper presents numerical modelling and an operational experiment to forge a slab ingot P40N from 55NiCrMoV7 tool steel and the procedure for the optimization of its production. The aim of the numerical simulation of forging was to verify the existing procedure of forging a plate from a conventional polygonal 8K forging ingot and a slab ingot with a polygonal shape of P40N surfaces. The effect of the shape of the ingot on the achievement of the required forging reduction and strain after the cross section of the forging of the plate, with final dimensions of approximately 1010 mm width × 310 mm thickness × 5350 mm length, was studied. The results obtained in the operational experiment showed satisfactory qualitative parameters of the steel forging from the slab P40N ingot which were in accordance with the predicted results of numerical simulations. The results indicated that in selected cases the use of a slab P40N ingot instead of the conventional polygonal 8K forging ingot can be considered in the production of certain plate-type forgings.
The prospects of processing blast furnace and steelmaking sludge using Waelz process in a laboratory rotary kiln is shown. The influence of varying thermal treatment modes, furnace atmosphere and type of reducing agents on the level of zinc reduction from sludges was analyzed. In general, the blast furnace sludge contains a high portion of iron (approx.48 wt. %) and can be reused as a charge after satisfactory zinc reduction. It was found that N- atmosphere and high content of the graphite or coke oven reducing agent in combination with high temperature can reduce the content of Zn in the sludge to 0.08 wt. % at 1200 °C for mixture of steelmaking and blast furnace sludge. A significant reduction in the Zn content to 0.66 wt. % occurs at 1100 °C. The content and type of reducing agent play an important role; graphite has shown a better reducing ability compared to coke oven dust. When nitrogen is used, zinc is reduced even without an additional reducing agent, since the carbon contained in the sludge is made use of for the reduction. In an air atmosphere, without the use of a reducing agent, there was no reduction in the Zn content.
The recovery of zinc from mixed steelmaking and blast furnace sludge was investigated through a direct comparison of the hydrometallurgical acetic acid leaching process and pyrometallurgical processing using coke dust as a reductive agent, with particular emphasis on the structure and functional properties of the resulting ZnO products. The mixed sludge contained 9.71 wt.% ZnO, with zinc occurring predominantly in the form of stable ferritic phases, mainly franklinite ((ZnFeII)Fe2O4). Hydrometallurgical treatment using 1 mol·dm−3 acetic acid resulted in only a limited relative decrease in Zn content (16.8%) based on solid-phase concentrations, as mainly readily soluble zinc phases were dissolved, while ferrite-bound zinc remained largely unaffected. In contrast, pyrometallurgical treatment of the sludge–coke dust mixture at 1200 °C enabled highly effective zinc volatilization, reducing the residual Zn content below 0.05 wt.% and resulting in a relative decrease in Zn content of 99.5% based on solid-phase concentrations. Characterization by XRD, FTIR, SEM, and EDS revealed substantial differences between the products obtained by the two processing routes. The pyrometallurgically prepared ZnO-rich product exhibited higher crystallinity, well-developed rod-like morphology, and substantially lower Fe and Pb contamination than the hydrometallurgically prepared material. In contrast, the hydrometallurgical product showed lower crystallinity and elevated Fe and Pb contents and therefore represented a highly contaminated ZnO-rich oxide mixture. Photocatalytic tests using Rhodamine B showed measurable but low activity of the pyrometallurgical product, with approximately 18% degradation after 120 min of UV irradiation, whereas the hydrometallurgical product was practically inactive. Overall, carbothermic treatment provided substantially more effective Zn removal than acetic acid leaching, although the recovered ZnO-rich product exhibited only limited photocatalytic activity.