Magnetic fraction isolated from steel furnace slag was tested as a component of Cu-free friction composites. The friction–wear performance and production of wear particles during their testing using a pin-on-disc tester against a cast iron disc were evaluated. To compare the effect of the magnetic fraction on the parameters studied, the composite with alumina and the composite with original steel furnace slag were also prepared and tested. All composites showed a comparable friction coefficient. The composite with original steel furnace slag, and the composite with a magnetic fraction showed higher wear resistance compared to the composite containing alumina. The positive effect of the magnetic fraction on the extent of the emission of wear particles was observed and explained by the decreased aggressiveness of this composite to the cast iron disc. The influence of the phase composition of the steel furnace slag and the magnetic fraction on the friction film formation was also indicated, and its effect on the production of wear particles was proposed.
The transition toward a circular economy requires innovative strategies for valorizing industrial by-products. This study investigates the potential of steelmaking furnace slag (SFS) as a low-cost adsorbent for the removal and recovery of nickel and copper ions from aqueous systems. The slag was characterized using XRF, XRD, SEM, FTIR, and thermal analyses, confirming the presence of reactive phases such as lime, periclase, and calcium silicates. Batch adsorption experiments revealed high sorption capacities (up to 147 mg·g−1) and were best described by the Langmuir isotherm and pseudo-second-order kinetic model, indicating chemisorption as the rate-limiting step. FTIR and SEM analyses demonstrated the formation of nickel and copper hydroxide/oxide phases, confirming surface precipitation mechanisms. Subsequent thermal treatment produced NiO- and CuO-enriched oxide systems with photocatalytic and antibacterial potential, while hydrometallurgical recovery using ammonia solutions achieved desorption efficiencies of 90–97%. The results highlight the dual role of SFS as an efficient sorbent for wastewater pre-treatment and as a secondary source of valuable metals, contributing to sustainable materials management and circular economy goals.
The recovery of zinc from mixed steelmaking and blast furnace sludge was investigated through a direct comparison of the hydrometallurgical acetic acid leaching process and pyrometallurgical processing using coke dust as a reductive agent, with particular emphasis on the structure and functional properties of the resulting ZnO products. The mixed sludge contained 9.71 wt.% ZnO, with zinc occurring predominantly in the form of stable ferritic phases, mainly franklinite ((ZnFeII)Fe2O4). Hydrometallurgical treatment using 1 mol·dm−3 acetic acid resulted in only a limited relative decrease in Zn content (16.8%) based on solid-phase concentrations, as mainly readily soluble zinc phases were dissolved, while ferrite-bound zinc remained largely unaffected. In contrast, pyrometallurgical treatment of the sludge–coke dust mixture at 1200 °C enabled highly effective zinc volatilization, reducing the residual Zn content below 0.05 wt.% and resulting in a relative decrease in Zn content of 99.5% based on solid-phase concentrations. Characterization by XRD, FTIR, SEM, and EDS revealed substantial differences between the products obtained by the two processing routes. The pyrometallurgically prepared ZnO-rich product exhibited higher crystallinity, well-developed rod-like morphology, and substantially lower Fe and Pb contamination than the hydrometallurgically prepared material. In contrast, the hydrometallurgical product showed lower crystallinity and elevated Fe and Pb contents and therefore represented a highly contaminated ZnO-rich oxide mixture. Photocatalytic tests using Rhodamine B showed measurable but low activity of the pyrometallurgical product, with approximately 18% degradation after 120 min of UV irradiation, whereas the hydrometallurgical product was practically inactive. Overall, carbothermic treatment provided substantially more effective Zn removal than acetic acid leaching, although the recovered ZnO-rich product exhibited only limited photocatalytic activity.