The article presents the results of primary crystallization, wear resistance and SEM studies of chromium cast iron inoculated with ferrotitanium and rare earth elements as a mischmetal inoculating mixture. Thermal-derivative analysis method was used to conduct studies of primary crystallization in two types of testers, namely ATD-C and ATD-Is, reflecting two different cooling speeds. Wear resistance tests were performed with the use of modified pin-on-disk method on Tribotester 3-POD device, where the samples were moving in circular motion in metal-mineral friction system. Silicon carbide was used as a counter sample. The studies allowed to determine the influence of selected inoculants on the microstructure and wear resistance of the studied samples. All characteristic crystallization temperatures of samples casted into ATD-Is testers increased, as well as wear resistance of each inoculated samples compared to the non-inoculated sample. It was proven that TiC and REE compounds are effective inoculants for chromium carbides and that REE compounds can work as underlay for TiC crystallization.
In recent years, white chromium cast iron has gained a well-settled position among wear-resistant materials. In recent times, chromium cast iron samples containing titanium have attracted attention. In cast iron samples, titanium combines with carbon and forms TiC particles, which may be form a crystallization underlay for eutectic M7C3 carbides and austenite. Accordingly, the inoculation process occurring in the crystallizing alloy should result in the proper, regular distribution of fine eutectic chromium carbides in the austenitic matrix. The presented research was conducted on 20% Cr hypoeutectic white cast iron with the addition of 0.5, 1, and 2% of Ti. Ti inoculation and the presence of TiC allowed for superior wear properties to be obtained. However, the conducted study revealed a significant decrease in the impact strength of examined alloys, especially for the cast iron samples with a high amount of Ti, in which the TiC compounds agglomerated. Titanium compounds accumulate in clusters and their distribution is irregular. Most of the TiC compounds were transported by the crystallization front into the center of the castings, where micropores were formed, meaning they were no longer effective crystallization underlays. In the authors’ opinion, the agglomerate formation is strictly connected with the appearance of bifilm defects in the casting microstructure. The conducted research shows how an incorrect volume of an additive may have negative influences on the properties of the casting. This is a vital issue not only from a technological point of view, but also for economic reasons.
Continuous improvement in the quality of castings is especially important since a cast without defects is a more competitive product due to its longer lifecycle and cheaper operation. Producing quality castings requires comprehensive knowledge of their production, crystallization process, and chemical composition. The crystallization of alloyed ductile iron (without the addition of magnesium) with oxide bifilm inclusions is discussed. These inclusions reduce the quality of the castings, but they are a catalyst for the growth of spheroidal graphite that crystallizes in their vicinity. The research was carried out for cast iron with a highly hyper-eutectic composition. Scanning electron microscopy and EDS analysis were used in the research. A detailed analysis of the chemical composition was also carried out based on the spectrometric method, weight method, etc. Based on the obtained results, a model of spheroidal graphite crystallization near bifilm inclusions was proposed. The surface of the analyzed graphite particles was smooth, which suggests a primary crystallization process. The phenomenon of simple graphite and bifilm segregation towards the heat center of the castings was also documented.
The aim of presented studies was to develop a new geometry of the overflow part of standard ATD-C tester for derivative thermal analysis in a way that it would allow to obtain samples for abrasion and mechanical properties tests in the same mould without the need of cutting them from a block of material. The pattern of new ATD-P tester has parts reflecting implemented samples. Computer simulations regarding initial verification of new tester were performed in NovaFlow software. Chromium cast iron melts were made for testing the sampler in real conditions and TDA analysis for casting material were conducted. The sandmix was prepared on silica sand matrix per the ALPHASET technology. This new solution greatly simplifies the preparations of materials difficult to machine.
The paper analyzes two types of alloyed cast iron used for pump impellers operated in mine working conditions. The research on corrosion resistance of two cast iron grades resistant to abrasive wear was presented. Tests were performed for chromium cast iron (HCCI) grade EN-GJN HV600 (XCr18) (acc. to EN 12513) and high-silicon cast iron HSCI Grade 1 (acc. to ASTM A 518/ A 518M - 99). Deposit mining is characterized by variable working conditions. Both types of cast iron are resistant to abrasive wear and are suitable for loaded elements (e.g. pump impellers). The paper presents a metallographic analysis of selected cast iron grades based on light microscopy. The chemical composition of the tested cast irons was determined with the Leco GDS 500 spectrometer; C and S content was determined with the CS125 Leco Carbon–Sulfur Determinator. The Si content for HSCI Grade 1 was determined by gravimetric method. Corrosion tests were performed under laboratory conditions. In-service tests of cast impellers were performed under real conditions (working mines applications). Corrosion resistance tests were measured with VoltaLab® Potentiostat (PGP 201). Performed tests resulted in the determination of the usefulness of materials used for dewatering pump impellers in mine working conditions. The results of laboratory tests were verified under the operating conditions of cast impellers. In the conditions of transporting a liquid-solid mixture at the moment of appearance of impurities (e.g. chlorine impurities) in the liquid, the impellers from cast iron HCCI revealed a tendency to pitting corrosion, which explains the exploitation results collected in the mining. After laboratory tests for sample from HCCI, the low value of breakdown potential Eb and repassivation Ecp was concluded which says about the absence of pitting corrosion resistance.