Ionic liquids have shown promising results in biomass pretreatment; however, an extensive water washing step is necessary. This fact increases not only the processing costs but also those associated with the ionic liquid recovery step. In this work, Eucalyptus globulus wood pretreated with two acetate-based ionic liquids, namely 1-ethyl-3-methylimidazolium acetate and choline acetate, has been washed with increasing volumes of water in order to analyze the influence of the amount of washing water used on the subsequent enzymatic hydrolysis stage and on the IL recovery costs. Vapor–liquid equilibria data of recovered ionic liquid/water mixtures have been determined to simulate the IL recovery step with Aspen Plus, calculating the operating costs using the Aspen Plus Economics Analyzer afterward. [Emim][OAc] was more efficiently washed and more effective toward wood pretreatment than [Ch][OAc]. Both IL/water systems were successfully modeled, and simulation studies showed that incremental volumes of water led to higher operating costs in the IL recovery step that are compensated with less IL makeup costs. Therefore, this work offers a technoeconomical analysis of the IL recovery step in a real biorefinery pretreatment process as a function of the volume of water used in the pretreated wood washing stage.
The lignocellulosic materials are promising feedstock to produce biofuels and bioproducts in the biorefinery framework. However, a pretreatment step is required to disrupt lignin-carbohydrate complex. In this work, the fractionation of Pinus radiata wood into its main components, cellulose-rich delignified solid, recovered lignin after precipitation, and soluble-in-black liquor hemicellulose, was studied. For this purpose, an organosolv process employing ethanol/water mixture as solvent in absence of a catalyst was carried out. The effects of operating conditions on delignified solid were evaluated by using a 23 central composite experimental design, being the responses delignified solid yield, delignification degree, hemicellulose content, and glucan content. The variables studied were temperature (170–200 °C), time (50–100 min), and ethanol concentration (40–60%). The increase of organosolv severity (temperature and time) and reduction of ethanol concentration favor the glucan enrichment of delignified solid, due to lignin removal and hemicellulose solubilization. A glucan content of more than 66% is obtained by applying temperature higher than 195 °C and time longer than 90 min, when 40 wt% alcohol concentration is used. The liquid fraction obtained during the organosolv process (black liquors) was used to recover lignin and hemicellulosic fractions solubilized. Furthermore, hemicellulose and lignin content of delignified solid was correlated with the thermal stability measured as T10%.