To avoid failures due to hydrogen embrittlement, it is important to know the amount of hydrogen absorbed by certain steel grades under service conditions. When a critical hydrogen content is reached, the material properties begin to deteriorate. The hydrogen uptake and embrittlement of three different carbon steels (API 5CT L80 Type 1, P110 and 42CrMo4) was investigated in autoclave tests with hydrogen gas (H2) at elevated pressure and in ambient pressure tests with hydrogen sulfide (H2S). H2 gas with a pressure of up to 100 bar resulted in an overall low but still detectable hydrogen absorption, which did not cause any substantial hydrogen embrittlement in specimens under a constant load of 90% of the specified minimum yield strength (SMYS). The amount of hydrogen absorbed under conditions with H2S was approximately one order of magnitude larger than under conditions with H2 gas. The high hydrogen content led to failures of the 42CrMo4 and P110 specimens.
20 December 2019 in BHM Berg- und Hüttenmännische Monatshefte
Microbiological methanation is investigated in an underground natural gas reservoir. Since H2 is involved in the process, hydrogen embrittlement of steel must inevitably be considered. Therefore, a routine for testing has been developed and a unique autoclave test bench was designed to simulate field conditions. The 2205 duplex stainless steel (UNS S31803) was investigated. Constant load tests (CLTs) and immersion tests with subsequent hydrogen analyses were performed. The specimens were exposed to different partial pressures of H2 under both dry and wet conditions (with brine). Additionally, the influence of CO2 under wet conditions was covered. Tests were performed at two different temperatures (25 °C and 80 °C) and lasted for 30 days. In general, the duplex stainless steel shows a good resistance to hydrogen embrittlement, but a significantly higher hydrogen uptake was obtained compared to other steel grades.