An electrochemical study of iron was carried out in KCl+LiCl+NaCl melt at 550ºC using a glassy carbon working electrode. Cyclic voltammetry showed that the Fe(II)/Fe(0) electron exchange is a soluble/insoluble reversible process. The diffusion coefficient of Fe(II) was calculated using cyclic voltammetry; 1.4×10-5 cm2 s-1. For the Fe(II)/Fe(III) red/ox reaction, analysis of the voltammograms suggests that the process is not reversible and is coupled with a chemical reaction. The stability of FeCl3 and the effect of equilibrium between FeCl3 and FeCl2 are also briefly discussed.
The Seebeck coefficient is reported for thermoelectric cells with gas electrodes and a molten electrolyte of one salt, lithium carbonate, at an average temperature of 750 °C. We show that the coefficient, which is 0.88 mV K−1, can be further increased by adding an inorganic oxide powder to the electrolyte. We interpret the measurements using the theory of irreversible thermodynamics and find that the increase in the Seebeck coefficient is due to a reduction in the transported entropy of the carbonate ion when adding solid particles to the alkali carbonate. Oxides of magnesium, cerium and lithium aluminate lead to a reduction in the transported entropy from 232 ± 12 to around 200 ± 4 J K−1 mol−1. This is of importance for design of thermoelectric converters.
We report Seebeck coefficients of electrochemical cells with molten carbonate mixtures as electrolytes and carbon dioxide|oxygen electrodes. The system is relevant for use of waste heat and off-gases with concentration of carbon dioxide different from air, as for example in the metallurgical industry. The coefficient is −1.25 mV K−1 for a nearly equimolar mixture of lithium and sodium carbonate with dispersed magnesium oxide at 750 °C, one bar total pressure and a pressure ratio of carbon dioxide to oxygen of 2:1. The value is slightly lower when sodium is replaced by potassium. The theoretical expression of the Seebeck coefficient was established using the theory of non-equilibrium thermodynamics. We used this expression to predict an increase to −1.4 mV K−1 when lowering the gas partial pressures to 0.015 and 0.2 bar, respectively, for carbon dioxide and oxygen, a gas composition that can represent that of the off-gases from a silicon furnace which we are concerned with. The absolute value of the Seebeck coefficient increases by 0.2 mV K−1 when the cell average temperature increases from 550 to 850 °C. The presence of a second component in the electrolyte increases the coefficient significantly above the values obtained with one component, compatible with a lowering of the transported entropy of the carbonate ion. A concentration cell, using the off-gas from the silicon furnace as anode gas and air as cathode gas, will add 0.14 V at 550°C to the absolute value of the potential. The series construction has the potential to offer a power density at matched load conditions in the order of 0.5 kW m−2.