1 October 2020 in Structures
Verified
Journal Article
Closed access
QWQiang Wang
Qiang Wang
HSHua-Lin Song
Hua-Lin Song
CLchunling lu
chunling lu
LJLing-Zhi Jin
Ling-Zhi Jin

1 October 2020 in Structures
Verified
Journal Article
Closed access
CLchunling lu
chunling lu
YXYi-Peng Xiao
Yi-Peng Xiao
QWQiang Wang
Qiang Wang
WZWan-Xu Zhu
Wan-Xu Zhu

8 March 2023 in Buildings
Verified
Journal Article
Open access
PDF file
QWQiang Wang
Qiang Wang
QWQin WeiYang
Qin WeiYang
CLchunling lu
chunling lu
Congested reinforcement may lead to difficulties with compacting concrete and reduce the connection efficiency. To overcome this problem, using large-diameter longitudinal rebar to replace medium-diameter longitudinal rebar to reduce the number of longitudinal rebars may be a useful mean. However, the seismic behavior of precast concrete (PC) columns with different-diameter longitudinal rebars was still unclear. In order to evaluate the influence of large-diameter longitudinal rebar replacement on the seismic behavior of PC columns, a series of large-scale reinforced concrete (RC) columns adopting similar concrete strength, longitudinal rebar ratio, and transverse rebar ratio was fabricated and tested. Six of the columns were prefabricated with grouted sleeve connections and the remaining two were cast in place (CIP) for reference. The longitudinal rebar diameter varied from 18 mm to 32 mm. A low-cycle reversed horizontal load was applied to study their seismic performance, including failure modes, load-bearing capacity, hysteresis behavior, stiffness degeneration, and energy-dissipation capacity. The test results showed that the PC column with large-diameter longitudinal rebar replacement performed similarly to CIP columns in general. The column with large-diameter longitudinal rebar suffered significant bond-slip between longitudinal rebar and concrete, especially for columns with a high axial compressive ratio of 0.6. It may be of detriment to the seismic behavior of the columns to some extent. Additionally, with the increase in the diameter of longitudinal rebar, the ductility and energy-dissipation capacity of PC columns were reduced slightly. In the grouted sleeve region, a local rigid zone was formed, making its overall lateral stiffness higher than that of corresponding CIP columns. It is recommended to extend the strengthening zone, with closer transverse reinforcement, to two times the column depth of the PC columns with grouted sleeve connections, as the plastic hinges may be shifted upward.

14 August 2020 in Materials
Verified
Journal Article
Open access
PDF file
QWQiang Wang
Qiang Wang
HSHua-Lin Song
Hua-Lin Song
CLchunling lu
chunling lu
WZWanxu Zhu
Wanxu Zhu
JHJia-Zhu Huang
Jia-Zhu Huang
In this study, a new method was proposed to study the relaxation properties of carbon fiber reinforced plastics (CFRP) fabric under axial tension. Under the condition of constant temperature and humidity, six groups of 168 h stress relaxation tests were conducted. Considering the influence of the prestress level, the size of CFRP cloth, and the surface coating of CFRP cloth on the relaxation performance, the measures to reduce the relaxation loss were proposed. The relaxation rate calculation model was established based on the test results of the authors and other scholars and was validated through comparisons with the test results. The results indicate that the relaxation rate of CFRP cloth was between 1.92% and 6.1%. When the prestress level was smaller than 0.3 fu, the relaxation rate of CFRP cloth decreased with the increase of prestress level. When the prestress level was greater than 0.3 fu, the relaxation rate increased with the increase of the prestress level. Under the same conditions, the relaxation rate of the CFRP specimens coated with glue was smaller than the uncoated samples by 3.21–6.28%. The calculation model could well estimate the relaxation rate of CFRP cloth.

9 July 2024 in Structural Concrete
Verified
Journal Article
Closed access
QWQiang Wang
Qiang Wang
XLXu‐Hua Liang
Xu‐Hua Liang
XLXin Liu
Xin Liu
SGShi‐Ping Guo
Shi‐Ping Guo
CLchunling lu
chunling lu

26 April 2024 in Materials
Verified
Journal Article
Open access
PDF file
CLchunling lu
chunling lu
XWXiangxiang Wang
Xiangxiang Wang
YNYuwen Ning
Yuwen Ning
KWKang Wen
Kang Wen
QWQiang Wang
Qiang Wang
In this paper, a thorough investigation is presented on the static and dynamic behaviors of a short-span cable-stayed bridge (CSB) incorporating steel and carbon fiber reinforced polymer (CFRP) hybrid cables. The study focuses on the world’s largest span and China’s first highway, CFRP CSB. The performance of the CSB was compared using numerical simulations under four different cable patterns: steel cables, CFRP cables, and steel, and two types of hybrid cables with different structural arrangements. The results indicate that the use of the use of CFRP cables in the long cable region in the short-span CSB project investigated in this study offers improved performance in terms of stability, seismic response, and reduced displacements. In comparison to CFRP cables, hybrid cables have demonstrated a reduction of 12% in the maximum vertical displacement of the main girder. On the other hand, the hybrid cables result in reduced maximum internal forces and longitudinal and lateral displacements of the main girders and towers compared to steel cables. The difference in the arrangement of CFRP cables in the long cable region or short cable region is not obvious under dead loads, but significant differences still exist between the CFRP cable bridges in the short cable region and the long cable region in terms of live load effects, temperature effects, and dynamic characteristics.