The high-temperature oxidation behavior of low-carbon steel (AISI 1015, AISI 8617, AISI 4115) was investigated over the temperature range from 600 to 1000 °C in humid air containing 25% water vapor. Mass gain of oxidation measurement was performed to study the oxidation kinetics. The microstructure, thickness, and composition of the oxide scale formed were investigated via optical microscope (OM), scanning electron microscope (SEM) equipped with an energy dispersive spectrometer (EDS), X-ray diffraction (XRD), and electron probe microanalyzer (EPMA). The oxidation process was performed from 2 to 100 min. As the oxidation time increased, the trend of mass gain per unit area switched from a linear to a parabolic law, regardless of the steel grade used. As the chromium content increased, the duration of time during which the oxidation rate followed a linear relationship decreased. In the low-alloy steel with higher chromium content, the thickness of the mixed oxide layer containing Cr increased and the oxidation rate decreased at all oxidation temperatures.
Three steel types (AISI 1020, AISI 8620, AISI 4120) with similar carbon content and different Cr content were used as test specimens to closely examine the effect of alloying elements for carbon penetration and diffusion on the steel surface during vacuum carburizing. The carbon mass gain according to the carburizing time was measured using a microbalance, and the average carbon flux, which is an indicator of the carbon penetration rate, was calculated using the measured weight as a variable. The outermost surface of the carburized specimen was observed by scanning electron microscopy (SEM) and Raman spectroscopy (RS), and the reason for the change in carburization rate according to the steel type was identified in relation to the equilibrium carbon contents calculated from Thermo-Calc. The overall carbon distribution and distribution of alloy elements on the outermost surface were quantitatively analyzed using an electron probe microanalyzer (EPMA). On the surfaces of the AISI 1020 and AISI 4120 carburized specimens, graphite layers and grain boundary carbide were formed during the carburizing process, which hindered the carburization rate, while no abnormal layer was observed on the surface of the AISI 8620 carburized specimens, so the overall carburization results were excellent.
Microstructural evolutions of AISI H13 steel during tempering were quantitatively investigated by scanning electron microscopy (SEM), x-ray diffractometer (XRD), impact test machine, rockwell hardness tester, ball-on-disk tester in order to describe the main mechanism of softening. Under the condition that the tempering time is 2 h, the hardness increases slightly as the tempering temperature increases, but decreases rapidly when the tempering temperature exceeds 500 °C, while the impact energy increases in proportion to the tempering temperature. Friction tests were conducted in dry condition with a load of 30 N, and the friction coefficient and wear rate according to tempering conditions were measured to prove the correlation with hardness and microstructure. In addition, primary tempering from 300 °C to 700 °C was performed at various times to establish a kinetic model to predict hardness under specific tempering conditions.
We used the chemical vapor deposition process to deposit carbon film at a high temperature (900 °C). The carbon films were deposited on AISI 1006 foils using an acetylene gas. We analyzed the carbon film deposited on the surface using Raman spectroscopy, scanning electron microscopy, and high-resolution transmission electron microscopy to define changes in the bonding structure of the carbon film. The results of Raman spectroscopy and high-resolution transmission electron microscopy revealed that as the acetylene flow rate increased, the shape of the deposited carbon film changed from graphene to graphite. In addition, in order to compare the quality of the carbon film in terms of mechanical and electrical properties, carbon films treated under various conditions were closely analyzed using nano-indenter and a sheet resistance meter. Therefore, the optimal condition (1 Torr-50 sccm) was selected in which graphene was uniformly deposited and had the lowest electrical resistance (500 Ω/sq) and highest hardness (12 GPa).
AlCrFeSi alloys have emerged as promising candidates for structural components requiring high strength, wear resistance, and thermal stability at elevated temperatures. To clarify the influence of processing conditions, elemental powders were synthesized by high-energy ball milling (HEBM) and consolidated via hot-press sintering (HPS) at 700 °C–1000 °C. Systematic characterization using XRD, SEM, hardness testing, and tribological evaluation revealed a strong dependence of densification and phase evolution on the sintering temperature. The optimum condition was found at 950 °C, where the alloys achieved nearly full densification (∼99.3%), refined microstructures with Al 13 Cr 2 and AlCr intermetallic phases, high hardness (∼495 HV), a reduced friction coefficient (0.37), and maximum fracture toughness of 4.1 MPa·m 1/2 . Further heating to 1000 °C caused grain coarsening and slight property degradation. These results highlight that precise control of the sintering temperature enables the fabrication of dense and wear-resistant AlCrFeSi alloys, providing useful guidance for the design of complex concentrated alloys for advanced high-temperature applications.
Decarburization during austenitization degrades the surface integrity and mechanical performance of tool steels, yet the quantitative influence of process pressure remains unclear. In this study, the effect of process pressure on the decarburization behavior of H13 tool steel was investigated. Specimens were austenitized at 920–1020 °C for 60 min under pressures ranging from 0.01 to 760 Torr. Carbon concentration profiles were measured by electron probe microanalysis, and hardness degradation and mass loss were evaluated. A one-dimensional diffusion model with a Robin boundary condition was applied to describe the coupled effects of carbon diffusion and surface reaction. High-vacuum conditions suppressed decarburization, whereas increasing pressure accelerated carbon loss, leading to deeper decarburized layers and pronounced hardness reduction. The model reproduced the experimental results and revealed a pressure-dependent transition in the dominant decarburization mechanism.
About Me
Gihoon Kwon is currently a Ph.D. student at Yonsei University and working at the Korea Institute of Industrial Technology.
Gihoon Kwon is currently a Ph.D. student at Yonsei University and working at the Korea Institute of Industrial Technology.