In this study, the effects of different precursor concentrations on the growth and characteristics properties of the zinc oxide (ZnO) nanorods (NRs) synthesized by using modified and conventional chemical bath deposition (CBD) methods were investigated. The morphologic, structural and optical properties of synthesized ZnO NRs with different precursor concentrations were studied using various characterization techniques. The experimental results show that the varying precursor concentration of the reactants has a remarkable and significant effect on the growth and characteristics properties of ZnO NRs. In addition, the characteristic properties of ZnO NRs grown using the modified method showed significantly improved and enhanced properties. The average length of grown ZnO NRs increased with increased precursor concentration; it can be seen that longer ZnO NRs have been investigated using the modified CBD methods. The ZnO NRs synthesized at 0.05 M using the modified method were grown with high aspect ratios than the ZnO NRs grown using conventional means which were 25 and 11, respectively. The growth rate increased with increased precursor concentration; it can be observed that a higher growth rate was seen using the modification CBD method. Furthermore, XRD results for the two cases reveal that the grown ZnO samples were a nanorod-like in shape and possessed a hexagonal wurtzite structure with high crystal quality. No other phases from the impurity were observed. The diffraction peaks along (002) plane became higher, sharper and narrower as precursor concentration increased, suggesting that the crystalline quality of ZnO NRs grown using the modified method was more enhanced and better than conventional methods. However, optical studies show that the transmittance at each concentration was more than two times higher than the transmittance using the modified CBD method. In addition, optical studies demonstrated that the ZnO NRs grown by using modified and conventional methods had a direct Eg in the range of (3.2–3.26) eV and (3.15–3.19) eV, respectively. It was demonstrated in two methods that ZnO NRs grown at a precursor concentration 0.05 M gave the most favorable result, since the NRs had best characteristic properties.
Ultraviolet (UV) photodetectors (PDs) based on high-quality well-aligned ZnO nanorods (NRs) were fabricated using both modified and conventional chemical bath deposition (CBD) methods. The modified chemical bath deposition (M-CBD) method was made by adding air bubbles to the growth solution during the CBD process. The viability and effectiveness of M-CBD were examined by developing UV PDs based on ZnO NRs. The ZnO nano-seed layer was coated on a glass substrate utilizing radiofrequency (RF) sputtering. The impact of the different growth-times on morphology, growth rate, crystal structure, and optical and chemical properties were investigated systematically using different characterization techniques, such as field-emission scanning electron microscopy (FE-SEM), X-ray diffraction (XRD) analysis, UV–VIS double beam spectrometer, and energy dispersive X-ray analysis (EDX), respectively. The Al/ZnO UV PDs based on ZnO nanorods were fabricated with optimum growth conditions through the two methods of preparation. This study showed that the synthesized ZnO NRs using the M-CBD method for different growth times possess better properties than the conventional method under similar deposition conditions. Despite having the highest aspect ratio and growth rate of ZnO NRs, which were found at 4 h growth duration for both methods, the aspect ratio of ZnO NRs using the M-CBD technique was comparatively higher than the conventional CBD method. Besides, the UV PDs fabricated by the M-CBD method at 5 V bias voltage showed high sensitivity, short response time, quick recovery time, high gain, low dark current, and high photocurrent compared with the UV PD device fabricated by the conventional CBD method.
Copper Sulfide (CuS) thin films were deposited onto a glass substrate using the Chemical Bath Deposition (CBD) technique. The chemical bath Precursors were made up of CuSO4, SC(NH2)2, and C4H6O6. Different parameters have been considered to specify the optimum conditions for fabricating CuS thin films, such as solution temperature, deposition time, pH level, and different precursor concentrations. It has been found that the optimum deposition time is 20 min at temperature 80 °C and pH = 11. The optimum precursor concentrations were 0.15 M, 0.2 M, and 0.1 M of CuSO4, SC(NH2)2, and C4H6O6, respectively. The structural properties of the thin film were studied using X-ray diffraction (XRD), and a single peak was observed for the thin film made at optimum conditions, while all other cases were amorphous. It is obvious from the optical characterization that the transmission spectra show a red-shift for the cases of increasing deposition time, bath temperature, C4H6O6 concentration, and pH. For the case of increasing CuSO4, blue shifts in the transmission spectra were observed. The energy band gap, resistivity, and activation energy of CuS thin films under optimum conditions are 2.35 eV, 0.7 Ω·cm, and 0.0152 eV, respectively.
One dimensional ZnO nanorods have been synthesized on flexible substrate. The substrate is Kapton Tape (KT). ZnO Nanorods are produced by using low cost chemical bath deposition method at low temperature. The investigation of the effect of substrate on the morphological, elementary composition, structural characteristics and Raman spectroscopy of ZnO nanorods has been done. Field emission scanning electron microscopy (FESEM), Energy Dispersive analysis (EDX), X-ray diffraction (XRD) and Raman spectroscopy measurements are employed to examine the morphological, compositional and structural characteristics with hexagonal wurtzite structure of the ZnO nanorods arrays. The results found that the average diameter of ZnO nanorods is found to be closely related to the substrate nature. It is concluded that the substrate can effect on the ZnO nanorods growth remarkably and the selective growth of ZnO nanorods is possible through the choice of the substrate. The crystallite size and the lattice constants of the synthesis ZnO nanorods are obtained based on the XRD data. The found results revealed that the increase in the crystallite size is strongly associated with the type of substrate.
1 August 2021 in Materials Science in Semiconductor Processing
Vertically aligned ZnO nanorods arrays were synthesized on glass substrates. ZnO seed layers were prepared on the glass substrate by RF Sputtering technique. ZnO nanorods synthesized using low-cost chemical bath deposition method at low temperature (95 ºC). The effect of the different growth time such as (0.5, 1, 2, 3, 4 and 5) h on the morphology, elemental chemical composition and structure of the ZnO nanorods were obtained systemically, and tested by Field emission scanning electron microscopy (FESEM), Energy dispersive analysis (EDX), and XRD measurements. The results found that the ZnO nanorods with hexagonal wurtzite structure grow vertically on the glass substrates. Most of the prepared samples have strong and sharp (002) peak intensities and the diffraction peaks (002) become higher and narrower as growth time increasing, obtaining that the ZnO crystalline quality became better with growth time increasing. The growth rate was decreased with increasing growth time, and the high aspect ratio was found at 4 h as a growth time. The size, length and crystalline size of the ZnO nanorods increase with increasing growth time. Furthermore, the ZnO nanorods vertically grow at (002) direction along the c-axis on the glass substrate, with elementary chemical compositions of zinc and oxygen only for all prepared samples.