Wastes are the sustainable sources of raw materials for the synthesis of new adsorbent materials. This study has as objectives the advanced capitalization of fly ash, by sulphuric acid activation methods, and testing of synthesized materials for heavy metals removal. Based on the previous studies, the synthesis parameters were 1/3 s/L ratio, 80 °C temperature and 10% diluted sulphuric acid, which permitted the synthesis of an eco-friendly adsorbent. The prepared adsorbent was characterized through SEM, EDX, FTIR, XRD and BET methods. Adsorption studies were carried out for the removal of Cd2+ ions, recognized as ions dangerous for the environment. The effects of adsorbent dose, contact time and metal ion concentrations were studied. The data were tested in terms of Langmuir and Freundlich isotherm and it was found that the Langmuir isotherm fitted the adsorption with a maximum adsorption capacity of 28.09 mg/g. Kinetic data were evaluated with the pseudo-first-order model, the pseudo-second-order model and the intraparticle diffusion model. The kinetics of cadmium adsorption into eco-friendly material was described with the pseudo-second-order model, which indicated the chemisorption mechanism.
Heat-resistant magnetic polymer composites were prepared by incorporating cerium-doped copper-nickel ferrite particles, having the general formula Ni1-xCuxFe1.92Ce0.08O4 (x: 0.0, 0.3, 0.6, 1.0), into a polyimide matrix. The effects of particle type and concentration on the thermal, magnetic, and electrical properties of the resulting composites were investigated. The samples were characterized by FTIR, scanning electron microscopy, X-ray diffractometry, thermogravimetric analysis, differential scanning calorimetry, vibrating sample magnetometer, and broadband dielectric spectroscopy. The composites exhibited high thermal stability, having initial decomposition temperatures between 495 and 509 °C. Saturation magnetization (Ms), magnetic remanence (Mr), and coercivity (Hc) were found in range of 2.37–10.90 emu g−1, 0.45–2.84 emu g−1, and 32–244 Oe, respectively. The study of dielectric properties revealed dielectric constant values of 3.0–4.3 and low dielectric losses of 0.016–0.197 at room temperature and a frequency of 1 Hz.
Novel hybrid inorganic CoFe2O4/carboxymethyl cellulose (CMC) polymeric framework nanobeads-type adsorbents with tailored magnetic properties were synthesized by a combination of coprecipitation and flash-cooling technology. Precise self-assembly engineering of their shape and composition combined with deep testing for cadmium removal from wastewater are investigated. The development of a single nanoscale object with controllable composition and spatial arrangement of CoFe2O4 (CF) nanoparticles in carboxymethyl cellulose (CMC) as polymeric matrix, is giving new boosts to treatments of wastewaters containing heavy metals. The magnetic nanobeads were characterized by means of scanning electron microscopy (SEM), powder X-ray diffraction analysis (XRD), thermogravimetric analysis (TG), and vibrational sample magnetometer (VSM). The magnetic properties of CF@CMC sample clearly exhibit ferromagnetic nature. Value of 40.6 emu/g of saturation magnetization would be exploited for magnetic separation from aqueous solution. In the adsorptions experiments the assessment of equilibrium and kinetic parameters were carried out by varying adsorbent dosage, contact time and cadmium ion concentration. The kinetic behavior of adsorption process was best described by pseudo-second-order model and the Langmuir isotherm was fitted best with maximum capacity uptake of 44.05 mg/g.
In this research, we reported on the formation of highly porous foam SrTiO3/NiFe2O4 (100−xSTO/xNFO) heterostructure by joint solid-state and sol-gel auto-combustion techniques. The colloidal assembly process is discussed based on the weight ratio x (x = 0, 25, 50, 75, and 100 wt %) of NiFe2O4 in the 100−xSTO/xNFO system. We proposed a mechanism describing the highly porous framework formation involving the self-assembly of SrTiO3 due to the gelation process of the nickel ferrite. We used a series of spectrophotometric techniques, including powder X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), transmission electron microscopy (TEM), N2 adsorption isotherms method, UV-visible diffuse reflectance spectra (UV-Vis DRS), vibrating sample magnetometer (VSM), and dielectric measurements, to investigate the structural, morphological, optical, magnetic, and dielectric properties of the synthesized samples. As revealed by FE-SEM analysis and textural characteristics, SrTiO3-NiFe2O4 nanocomposite self-assembled into a porous foam with an internally well-defined porous structure. HRTEM characterization certifies the distinctive crystalline phases obtained and reveals that SrTiO3 and NiFe2O4 nanoparticles were closely connected. The specific magnetization, coercivity, and permittivity values are higher in the 75STO/25NFO heterostructure and do not decrease proportionally to the amount of non-magnetic SrTiO3 present in the composition of samples.