We report herein high-resolution x-ray diffraction measurements of basal plane bending of homoepitaxial single-crystal diamond (SCD). The results reveal that growth parameters such as temperature, growth time and basal plane bending of the substrate affect the basal plane bending of SCD. First, the basal plane bending of SCD depends mainly on the substrate itself. The basal plane bending of SCD becomes more severe with increasing basal plane bending of the substrate and this type of basal plane bending cannot be recovered. The SCD growth experiments show that the basal plane bending increases at high temperature and with increasing growth time. Finally, to understand the mechanism behind basal plane bending, we investigate the substrate-surface temperature distribution as a function of basal plane bending of SCD fabricated by chemical vapour deposition (CVD). This allows us to propose a bending model and understand the origin of basal plane bending. The results indicate that an uneven temperature distribution on the substrate surface is the main cause of the CVD diamond base-plane bending.
High-purity SiC powder is an important feedstock for SiC crystal growth, but thermal-field regulation becomes difficult during large-batch synthesis. This study examined an α-SiC powder-synthesis furnace with upper and lower induction-coil groups through numerical simulations and 70 kg synthesis experiments. A representative two-dimensional axisymmetric model was used to compare eight cases with different coil-turn or numerical power allocations. Redistributing the coil turns changed , , volumetric Joule heat density, , and the resulting temperature and calculated gas-phase velocity-magnitude fields. From C01 to C04, the maximum calculated temperature decreased from 2501.10 to 2359.13 K, while decreased from 242.57 to 76.20 K. Increasing the upper-coil numerical power raised the temperature level while reducing to 152.41 K. Increasing the lower-coil numerical power also raised the temperature level, but increased to 292.26 K. Equal-total-power comparisons showed that axial power allocation affected and . XRD identified 6H-SiC as the detected crystalline phase in both analyzed middle-region specimens, although X-ray-amorphous carbon could not be excluded. The specimens also differed in macroscopic appearance, measured impurity concentrations, and local nitrogen concentration profiles. Because the experimental conditions were maintained nominally unchanged except for the upper-coil current, these specimen-level differences may be associated with altered internal thermal conditions. Such changes may affect local equilibrium, supersaturation, and species transport, providing a possible link to the observed material differences. The numerical results identify coil-turn allocation and axial power allocation as variables for regulating the calculated furnace fields.