The morphology of magnetic materials has a great influence on the properties, which is attributed to the magnetic anisotropy of the materials. Therefore, it is worth studying the fabrication of the aligned fiber and the change of its domain distribution. Nanoparticles and nanofibers were prepared by the hydrothermal and electrospinning methods, respectively. At the same time, the arranged nanofibers were collected by the drum collecting device. After the same annealing at 700 °C, it was found that the diameter of fibers collected by different collecting drums is similar. By studying the hysteresis loops of nanoarrays, it was found that they had strong anisotropy. The easy axis was parallel to the long axis, the Hc and Mr of the easy axis and the hard axis were 1330.5 Oe, 32.39 Am2/kg, and 857.2 Oe, 24.8 Am2/kg, respectively. Due to the anisotropy of the shape and the interaction between the particles, the Hc could not be enhanced. Therefore, the Ms and Hc of the nanoparticles were 80.23 Am2/kg and 979.3 Oe, respectively. The hysteresis loop and the change of magnetic moment during the demagnetization of the CoFe2O4 nanofiber array were simulated via micromagnetic software. The simulated Hc was 1480 Oe, which was similar to the experimental value.
In order to enhance the resistance of superalloys to high-temperature molten chloride salt corrosion, Fe-Al coatings were prepared on 310S and 347H stainless-steel surfaces via pack aluminizing. Then, the coatings were annealed at different temperatures to explore the influence of temperature on their phase constitution, microstructure, microhardness, and corrosion resistance. The results showed that the annealing temperature had a considerable effect on the corrosion resistance of the Fe-Al coatings, which was related to the change in the phase composition of the coatings that occurred due to the annealing treatment. The growth rate of the coating on 347H steel was higher than that on 310S steel, and their thicknesses from aluminizing at 800 °C for 20 h were 209.6 and 153.5 µm, respectively. When annealing at 900 °C for 30 h, the phase composition of the coatings was completely transformed into (Fe, Cr, Ni) Al. The corrosion loss rate of the annealed coating was clearly reduced, the loss rate of the 310 coating was 6.0 and −0.25 mg/cm2 before and after annealing at 900 °C and that of the 347 coating was 4.89 and −0.7 mg/cm2 before and after annealing at 750 °C, respectively. The two coatings showed good corrosion resistance to molten chloride salts, as demonstrated by the oxide scale (Al2O3) that formed on the surface, which had a thickness of about 30~40 µm.