The effect of deformation temperature on the mechanical properties of 1-GPa-grade TRIP steels with different retained austenite (γR) morphologies was studied. The temperature dependence on the deformation-induced martensitic transformation behavior was also investigated. The uniform elongation below room temperature was relatively large in the needle-like γR steel, whereas the tensile strength at each temperature was almost the same as it was independent of the γR morphology. The better tensile strength–uniform elongation balance was obtained at 373 K for the needle-like γR steel and at 473 K for blocky γR one. The mechanical stability of γR was higher in the needle-like γR steel, according to the x-ray diffraction experiments. γR was mechanically stable with increasing temperature, but its volume fraction decreased at temperatures above 473 K because of the deformation-induced bainitic transformation. In this paper, the quantitative conditions of deformation-induced transformation to obtain better uniform elongation in the 1-GPa-grade TRIP steels are summarized from the viewpoints of the volume fraction of deformation-induced martensite and the transformation rate.
The better uniform elongation of the 1 GPa-grade TRIP-aided multi-phase steel with retained austenite (γR) shape of needle-like was discussed by in situ neutron diffraction experiments during tensile test. The better uniform elongation can be ascribed by not only the deformation-induced martensitic transformation of γR but also the deformation behavior of γR and ferrite phase. Especially, the tensile deformation behavior of γR is found to be closely associated with both of the stress-strain curve and the deformation-induced martensitic transformation of γR. The tensile deformation behavior of γR should be considered as one of the conditions to obtain better TRIP effect.
Deformation-induced martensitic transformation (DIMT) during tensile or compressive deformations of the bainitic steels with various carbon content (0.15 %C, 0.25 %C, 0.62 %C) was studied. The initial microstructure before the deformation tests was prepared by the austempering at 400 °C to obtain bainitic structure consisting of bainitic ferrite and retained austenite. The volume fraction of the retained austenite was larger in the bainitic steel with the larger carbon content. In all of the bainitic steels, the tensile deformation exhibited larger work hardening than the compression. This difference indicates the suppression of the DIMT at the compression, and actually the measurements of electron back scattering diffraction (EBSD) confirmed the less reduction of retained austenite at the compression of all the bainitic steels. Additionally, the steel with the highest carbon content was examined by in situ neutron diffraction and clarified the difference similar to that obtained by the EBSD measurement. The regression of the relation between the fraction of austenite and applied strain with the conventional empirical equation revealed that the kinetic of DIMT is strongly dependent with the stress polarity, but not significantly changed by the carbon content. The mechanism of the DIMT dependence of the stress polarity was discussed with the deformation texture and the crystallographic orientation dependence of DIMT.
Ni-free austenitic steels containing high nitrogen have been developed to protect against earth resource. High nitrogen steels (HNS) have a lot of advantages, e.g., HNS have high strength, corrosion resistance, toughness, work hardening rate and large rocking parameter in the Hall-Petch equation. On the other hand, it is difficult to fabricate HNS by IM method under 0.1 MPa and to work at room temperature. We have tried to make HNS by combined use of metal injection molding method (MIM) and nitrogen absorption method. Powder compositions used was Fe-17Cr-12Mn-3Mo.The benefit of this method is to make metal parts in near net shape. In order to use this method, we should know the sintering heat schedule, timing for introducing nitrogen gas, gas pressure and setter material etc. Therefore, the shrinkage rate, density and the solution-treated microstructure of MIM compacts were examined to find out the optimum conditions.