The article presents research on the comminution of copper ore in a self-constructed mill using high-pressure water jet energy to investigate the usefulness of such a method for comminuting copper ore. As a result, ore particles are obtained that are characterized by appropriate comminution and a significant increase in their specific surface, in turn allowing for potential further processing of the mineral. A comparative analysis of the efficiency of copper ore comminution, primarily taking into account the unit energy consumption and the efficiency of the milling process, clearly indicates that the energy absorption of hydro-jet material comminuting is lower than during mechanical grinding, e.g., in a planetary ball mill. The applicability of the technique depends on the brittle nature of the host rock, e.g., it is especially appropriate for sandstone and shale ores.
1 January 2009 in Archives of Civil and Mechanical Engineering
This paper presents an original method for the comminution of polymetallic nodules in a hydro-jet mill of our own design, having the water jet pressure in the range of 70–200 MPa. The best comminution results are ensured by equipping the mill with a water jet having a diameter dw = 0.7 mm and a comminution-homogenization tube having a diameter dh = 2.4 mm, and by setting a distance s = 10 mm from the outlet of the homogenization tube to the comminuting disc. Particles of concretions comminuted under such conditions are characterized by a fairly regular isometric shape and favorable morphology represented by intense development of the specific surface.
This paper presents an original method for the micronization of coal particles in a hydro-jet mill, which allows effective comminuting of coal in the pressure range of 100–250 MPa, at a variable water flow rate of 0.2–0.5 dm3/s. The discussed high-pressure water jet mill (HPWJM) allows the comminution of standard fines, with a grain size up to 2 mm, and at a relatively high comminuting efficiency of 8 to 55 g/s. In addition, the paper presents energy-consumption ratios, and indicates the advantage of this method over mechanical grinding in a planetary ball-mill. At optimum conditions, coal comminution at an efficiency of Qc = 38.4 g/s and at an energy input of EH = 1.1 MJ/kg provides an average particle size of about 40 µm. The degree of comminution was further improved by applying roto-turbulent micronization, which resulted in an average size of comminuted coal particles of only 17 µm. As an additional result, the actual surface area of the particles increased by 10–30 thousand times when compared to ground fines—this fact is of significance for the application of micronized particles in quasi-liquid coal-water fuel.
10 September 2010 in Journal of Manufacturing Science and Engineering
Novel method for the 3D shaping of different materials using a high-pressure abrasive water jet is presented in the paper. For the steering movement process of the jet, a principle similar to the raster image way of record and readout was used. However, respective colors of pixels of such a bitmap are connected with adequate jet feed rate that causes erosion of material with adequate depth. Thanks to that innovation, one can observe spatial imaging of the object. Theoretical basis as well as spatial model of material shaping including steering program is presented in. There are also presented experimental erosion results as well as practical examples of the object’s bas-relief made of metal.
10 December 2019 in Materiały Wysokoenergetyczne / High Energy Materials