Andreas Lümkemann

Dr. Andreas Lümkemann


Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
22 September 2020 in Coatings
Verified
Journal Article
Open access
PDF file
ASAsad Alamgir Shaikh
Asad Alamgir Shaikh
MYMaxim Yashin
Maxim Yashin
ABAndrei Bogatov
Andrei Bogatov
MVMart Viljus
Mart Viljus
RTRainer Traksmaa
Rainer Traksmaa
Vitali PodgurskyVitali Podgursky
Vitali Podgursky
Mechanical and tribological properties of the hard-multilayer TiN-AlTiN/nACo-CrN/AlCrN-AlCrO-AlTiCrN coating deposited on WC-Co substrate were investigated. The sliding tests were carried out using ball-on-disc tribometer at room (25 °C) and high temperatures (600 and 800 °C) with Al2O3 balls as counterpart. Nano-scratch tests were performed at room temperature with a sphero-conical diamond indenter. The surface morphology and chemical composition were investigated with scanning electron microscopy (SEM), energy-dispersive spectrometry (EDS) and in-situ high-temperature X-ray diffraction (HT-XRD). The phase transition from fcc-(Al,Cr)2O3 into α-(Al,Cr)2O3 was observed at about 800 °C. The results of the tribological tests depends on the temperature, the lowest apparent and real wear volumes were observed on the coating after the test at 800 °C along with the smallest coefficient of friction (COF). The plastic deformation of the coating was confirmed in sliding and nano-scratch tests. The nano-scratch tests revealed the dependence of COF value on the temperature of the sliding tests.

6 May 2020 in Materials
Verified
Journal Article
Open access
PDF file
JDJosef Daniel
Josef Daniel
RŽRadek Žemlička
Radek Žemlička
JGJan Grossman
Jan Grossman
ALAndreas Lümkemann
Andreas Lümkemann
PTPeter Tapp
Peter Tapp
TFTomas Fort
Tomas Fort
Protective hard PVD coatings are used to improve the endurance of the tools exposed to repeated impact load, e.g., fine blanking punches. During the fine blanking process, a coated punch repeatedly impacts sheet metal. Thus, the coating which protects the punch surface is exposed to the dynamic impact load. On the other hand, the laboratory method of dynamic impact testing is well known and used for the development and optimization of protective coatings. This paper is focused on the comparison of tool life and lifetime of the industrial prepared PVD coatings exposed to repeated dynamic impact load in the industrial fine blanking process and the laboratory dynamic impact testing. Three different types of protective coatings were tested and the results were discussed. It was shown that the lifetime of coated specimens in both the fine blanking and the dynamic impact processes was influenced by similar mechanical properties of the protective coatings. The qualitative comparison shows that the lifetime obtained by the dynamic impact test was the same as the lifetime obtained by the industrial fine blanking process. The laboratory impact test appears to be a suitable alternative for the optimisation and development of protective PVD coatings for punches used in the industrial fine blanking process.

18 April 2022 in Coatings
Verified
Journal Article
Open access
PDF file
ASAsad Alamgir Shaikh
Asad Alamgir Shaikh
ABAndrei Bogatov
Andrei Bogatov
TJTaivo Jõgiaas
Taivo Jõgiaas
MVMart Viljus
Mart Viljus
TRTaavi Raadik
Taavi Raadik
Vitali PodgurskyVitali Podgursky
Vitali Podgursky
The focus is on the oxidation resistance and tribological performance of ta-C and Al2O3/ta-C coatings. The wear tests were carried out on the ball on disc tribometer at room (25 °C) and high (400, 450 and 500 °C) temperatures in ambient air with Si3N4 balls as counterbodies. Scanning electron microscopy and Raman spectroscopy were used to analyze the surface morphology and chemical bonding, respectively. The Al2O3/ta-C coating exhibited better oxidation resistance and tribological performance at elevated temperatures than the ta-C coating. The Raman analysis revealed that a thin alumina layer suppresses structural changes in the ta-C coating at elevated temperatures, thus preserving the sp3 content.

23 April 2021 in Coatings
Verified
Journal Article
Open access
PDF file
Vitali PodgurskyVitali Podgursky
Vitali Podgursky
ASAsad Alamgir Shaikh
Asad Alamgir Shaikh
MYMaxim Yashin
Maxim Yashin
TJTaivo Jõgiaas
Taivo Jõgiaas
MVMart Viljus
Mart Viljus
ABAndrei Bogatov
Andrei Bogatov
The study investigates thermal stability and high temperature tribological performance of a-C:H:Si diamond-like carbon (DLC) coating. A thin alumina layer was deposited on top of the a-C:H:Si coating to improve the tribological performance at high temperatures. The a-C:H:Si coating and alumina layer were prepared using plasma-activated chemical vapour deposition and atomic layer deposition, respectively. Raman and X-ray photoelectron spectroscopy were used to investigate the structures and chemical compositions of the specimens. The D and G Raman peaks due to sp2 bonding and the peaks corresponding to the trans-polyacetylene (t-Pa) and sp bonded chains were identified in the Raman spectra of the a-C:H:Si coating. Ball-on-disc sliding tests were carried out at room temperature and 400 °C using Si3N4 balls as counter bodies. The a-C:H:Si coating failed catastrophically in sliding tests at 400 °C; however, a repeatable and reproducible regime of sliding with a low coefficient of friction was observed for the Al2O3/a-C:H:Si coating at the same temperature. The presence of the alumina layer and high stress and temperature caused structural changes in the bulk a-C:H:Si and top layers located near the contact area, leading to the modification of the contact conditions, delivering of extra oxygen into the contact area, reduction of hydrogen effusion, and suppression of the atmospheric oxidation.

25 February 2023 in Coatings
Verified
Journal Article
Open access
PDF file
JDJosef Daniel
Josef Daniel
RŽRadek Žemlička
Radek Žemlička
MAMostafa Alishahi
Mostafa Alishahi
PKPavla Karvánková
Pavla Karvánková
PSPavel Souček
Pavel Souček
PVPetr Vašina
Petr Vašina
AlCrN coatings, which are characterized by high hardness and good wear resistance, are often used for drilling, milling, and punching tools. Therefore, the study of the behaviour of these coatings under cyclic impact loading is essential for their optimization. Our previous work has focused on the study of the composition and microstructure of AlCrN coatings prepared using a cathodic arc deposition system with a SCIL® controller that controls the average ion energy per deposited atom (Ed). Two sets of coatings were prepared in two different modes, with a metal target and with a poisoned target. The chemical compositions of the coatings were very similar regardless of their deposition conditions, but the structure and mechanical properties of the coatings depended strongly on Ed. The present work focused on the scratch adhesion and impact wear of these two sets of AlCrN coatings. The lifetimes of both sets of samples under repeated dynamic impacts were tested using a dynamic impact tester with a WC-Co ball. It was shown that the impact behaviour of the coatings prepared in the metallic regime does not depend on the deposition conditions. However, the impact behaviour of the coatings deposited in poisoned mode was improved by increasing Ed.

15 April 2026 in Defect and Diffusion Forum
Verified
Journal Article
Open access
PDF file
NPNils Paucke
Nils Paucke
MBMartin Beutner
Martin Beutner
ALAndreas Lümkemann
Andreas Lümkemann
KTKeith Thomas
Keith Thomas
MUMartin Učík
Martin Učík
MHMatthias Hackert-Oschätzchen
Matthias Hackert-Oschätzchen
Dry machining of gears demands advanced coating technologies to withstand high thermal and mechanical stresses. In this study, AlCrN coatings were deposited using the newly developed Focused Magnetron Sputtering (FMS) process and compared with conventional Cathodic Arc Evaporation (CAE)-AlCrN and boroncontaining CAE-AlCrBN coatings. XRD analysis showed that FMS produced a finegrained crystal structure with half the full width at half maximum (FWHM) of CAE-AlCrN. Stressoptimised deposition allowed a 60 % higher coating thickness with improved adhesion. Analogy gear hobbing tests (fly cutting tests) demonstrated that FMS-AlCrN had 52 % lower crater wear than CAE-AlCrN, while CAE-AlCrBN also improved crater wear resistance due to boroninduced grain refinement. However, both finegrained coatings exhibited increased flank wear compared to the coarse-grained CAE-AlCrN coating. The results show that FMS enables the production of dense, fine-grained coatings with superior adhesion and crater wear resistance, highlighting its potential for dry gear hobbing. Further optimisation of hardness and microstructure is required to balance crater and flank wear behaviour.