Ruiming Ren

Ruiming Ren


Research Focus & Metrics

Academic Career Length

9Years (2018-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
8 October 2019 in Materials
Verified
Journal Article
Open access
PDF file
CLchun peng liu
chun peng liu
XZXiujuan Zhao
Xiujuan Zhao
PLpengtao liu
pengtao liu
JPJin-Zhi Pan
Jin-Zhi Pan
RRRuiming Ren
Ruiming Ren
To investigate the relationship between surface microstructure and wear mechanism in D2/U71Mn wheel-rail material under different contact stress conditions, rolling wear tests using a GPM-40 wear machine to simulate the wheel-rail operation was performed. After wear tests, an optical microscope (OM), scanning electron microscope (SEM) and micro-hardness testers were used to characterize the microstructure and fatigue wear cracks. The results show that the thickness of the plastic deformation layer and surface hardness is increased with the increase of contact stress. Under high contact stress condition (1200 MPa), the severe plastic deformation layer led to the formation of fatigue wear of wheel-rail samples. Under a contact stress of 700 MPa, the wear mechanism of samples is adhesive wear and wear rate is low. With the increase of contact stress, the fatigue cracks are gradually severe. Under a contact stress of 1200 MPa, the wear mechanism of samples becomes fatigue wear and the fatigue wear cracks cause the increase of wear rate. The fatigue wear can accelerate the wear failure of wheel-rail samples. The fatigue wear cracks of wheel samples are severer than that of rail samples due to both the rate of plastic strain and the content of proeutectoid ferrite.

3 December 2018 in Journal of Iron and Steel Research International
Verified
Journal Article
Closed access
PDF file
CLChun-Peng Liu
Chun-Peng Liu
XZXiu-Juan Zhao
Xiu-Juan Zhao
PLPeng-Tao Liu
Peng-Tao Liu
CXChong Xu
Chong Xu
RRRuiming Ren
Ruiming Ren

15 February 2020 in Wear
Verified
Journal Article
Closed access
CLChun-Peng Liu
Chun-Peng Liu
PLPeng-Tao Liu
Peng-Tao Liu
JPJin-Zhi Pan
Jin-Zhi Pan
CCChun-Huan Chen
Chun-Huan Chen
RRRuiming Ren
Ruiming Ren

29 November 2020 in Materials
Verified
Journal Article
Open access
PDF file
PLpengtao liu
pengtao liu
YHYizhu He
Yizhu He
CLchun peng liu
chun peng liu
XZXiujuan Zhao
Xiujuan Zhao
RRRuiming Ren
Ruiming Ren
A GPM-30 fatigue machine was used to investigate the influence of surface ultrasonic rolling (SURT) on the rolling contact fatigue (RCF) life of D2 wheel steel. The experimental results present that the RCF life of the grinding processing sample is 4.1 × 105 cycles. During the RCF process, the flaking of the fine grain layer and high surface roughness of the grinding processing sample cause the production of RCF cracks. When the samples are treated by SURT with 0.2 MPa and 0.4 MPa, the RCF life is 9.2 × 105 cycles and 9.6 × 105 cycles, respectively. After SURT, the surface roughness of the samples is reduced, and a certain thickness of gradient-plastic-deformation layer and a residual-compressive-stress layer are produced. These factors lead to the improvement of the RCF property. However, when the static pressure increases to 0.6 MPa during SURT, the RCF life of the sample is reduced during RCF testing. The micro-cracks, which are formed during SURT, become the crack source and cause the formation of RCF cracks, decreasing of the RCF life.

7 May 2021 in Journal of Materials Engineering and Performance
Verified
Journal Article
Closed access
PDF file
CSChong Su
Chong Su
XSXinghua Sang
Xinghua Sang
SNShanjin Niu
Shanjin Niu
RRRuiming Ren
Ruiming Ren

6 April 2020 in Ironmaking & Steelmaking: Processes, Products and Applications
Verified
Journal Article
Closed access
CLChun-Peng Liu
Chun-Peng Liu
PLPeng-Tao Liu
Peng-Tao Liu
JPJin-Zhi Pan
Jin-Zhi Pan
CCChun-Huan Chen
Chun-Huan Chen
RRRuiming Ren
Ruiming Ren
In this work, the influence of original microstructure on wear property of ER9 wheel steel is studied by GPM-40 rolling wear tester. The pearlite + proeutectoid ferrite (P+F) sample exhibits the lower wear loss than the tempered sorbite (TS) sample at different cycles. However, the TS sample has better fatigue wear resistance than the P+F sample. High wear loss and more uniform plastic deformation of the TS sample can inhibit the formation of fatigue wear cracks. During rolling-sliding wear process, for the P+F sample, the high surface hardness and the pearlite colonies/proeutectoid ferrite are the main reasons to cause the initiation of fatigue cracks. The formation of an interface of hardening layer causes the propagation of cracks easily. These factors lead to a large amount of fatigue wear cracks be formed at the P+F sample surface.