Transesterification of palm olein with glycerol can increase the functionality by introducing additional hydroxyl groups to the triglyceride structure, an advantage compared to using palm olein directly as feedstock for producing palm‐based polyol. The objective of this study was to synthesize transesterified palm olein‐based polyol via a three‐step reaction: (1) transesterification of palm olein, (2) epoxidation and (3) epoxide ring opening. Transesterification of palm olein yielded approximately 78 % monoglyceride and has an hydroxyl value of approximately 164 mg KOH g−1. The effect of formic acid and hydrogen peroxide concentrations on the epoxidation reaction was studied. The relationships between epoxide ring‐opening reaction time and residual oxirane oxygen content and hydroxyl value were monitored. The synthesized transesterified palm olein‐based polyol has hydroxyl value between 300 and 330 mg KOH g−1 and average molecular weight between 1,000 and 1,100 Da. On the basis of the hydroxyl value and average molecular weight of the polyol, the transesterified palm olein‐based polyol is suitable for producing rigid polyurethane foam, which can be designed to exhibit desirable properties. Rigid polyurethane foams were synthesized by substituting a portion of petroleum‐based polyol with the transesterified palm olein‐based polyol. It was observed that by increasing the amount of transesterified palm olein‐based polyol, the core density and compressive strength were reduced but at the same time the insulation properties of the rigid polyurethane foam were improved.
The development of bio-polyol from vegetable oil and its derivatives is gaining much interest from polyurethane industries and academia. In view of this, the availability of methyl oleate derived from palm oil, which is aimed at biodiesel production, provides an excellent feedstock to produce bio-polyol for polyurethane applications. In this recent study, response surface methodology (RSM) with a combination of central composite rotatable design (CCRD) was used to optimise the reaction parameters in order to obtain a maximised hydroxyl value (OHV). Three reaction parameters were selected, namely the mole ratio of epoxidised methyl oleate (EMO) to glycerol (1:5–1:10), the amount of catalyst loading (0.15–0.55%) and reaction temperature (90–150 °C) on a response variable as the hydroxyl value (OHV). The analysis of variance (ANOVA) indicated that the quadratic model was significant at 98% confidence level with (p-value > 0.0001) with an insignificant lack of fit and the regression coefficient (R2) was 0.9897. The optimum reaction conditions established by the predicted model were: 1:10 mole ratio of EMO to glycerol, 0.18% of catalyst and 120 °C reaction temperature, giving a hydroxyl value (OHV) of 306.190 mg KOH/g for the experimental value and 301.248 mg KOH/g for the predicted value. This result proves that the RSM model is capable of forecasting the relevant response. FTIR analysis was employed to monitor the changes of functional group for each synthesis and the confirmation of this finding was analysed by NMR analysis. The viscosity and average molecular weight (MW) were 513.48 mPa and 491 Da, respectively.
2 March 2023 in Biomass Conversion and Biorefinery
The Lewis acid ring-opening of epoxidized vegetable oils (EVO's) in the presence of tetrahydrofuran (THF) gives rise to polyether polyol co-polymers p(THF-stat-EVO). The effect of Lewis acid, vegetable oil substrate (epoxidised methyloleate EMO, epoxidised cocoa butter ECB, and epoxidised palm oil EPO) and conditions (concentration, temperature and time) on the molecular weight, polydispersity, hydroxyl value and thermal properties of the p(THF-stat-EVO) macromonomers was determined. Elastomeric polyurethanes were prepared from p(THF-stat-EVO) macromonomers and MDI and their mechanical and thermal properties determined. The properties of the polyurethane derived from p(THF-EPO) were compared to that derived from the homopolymer of epoxidised palm oil (EPO) prepared by Lewis acid ring-opening in the absence of THF. The co-polymer incorporating THF gave rise to a material with significantly greater tensile strength [p(THF-EPO-MDI) = 9.1 MPa, p(EPO-MDI) = 1.5 MPa] and elongation at break [p(THF-EPO-MDI) = 425%, p(EPO-MDI) = 70%] with little compromise on thermal stability [p(THF-EPO-MDI) Tdecomp10% = 378 °C, Tdecomp50% = 414 °C, p(EPO-MDI) Tdecomp10% = 379 °C Tdecomp50% = 424 °C].
12 August 2020 in European Journal of Lipid Science and Technology