The current research unfolds the effect of block lengths, microdomain morphology and stereocomplexation on the mechanical properties of PLA-b-PCL-b-PLA triblock copolymers where PCL is involved to improve the poor extensibility of PLA. The linear triblock copolymers PLLA-b-PCL-b-PLLA and PDLA-b-PCL-b-PDLA (PLLA:poly (L-lactic acid) and PDLA:poly (D-lactic acid)) are made by two step ring opening polymerization and blended in a 1 : 1 ratio to achieve stereocomplex blends where the molecular weight of the terminal and the mid segment is tailored. The mechanical strength and elongation at break range from 13 MPa to 36 MPa and 540 to 950%, respectively, for the triblock copolymers with varied block lengths. Such wide-ranged mechanical properties are ascribed to the morphology of the self-assembled nanostructure of triblock copolymers as corroborated with the small angle X-ray scattering (SAXS) results. To render it industrially viable, the process of triblock copolymer synthesis is scaled up to ∼500 g batch followed by its processing using a twin-screw extruder to make a filament which is used for 3D printing of a mesh-type scaffold. The synthesized materials are tested for their biocompatibility by performing MTT assay using rat bone osteosarcoma (UMR-106) cells which renders them as potential biomaterials.
Strain‐induced crystallization (SIC) in natural rubber (NR) near crack tips significantly enhances crack growth resistance, but understanding the interplay between local strain field and crystallization remains challenging due to confined and heterogeneous characteristics. Using micro‐scale digital image correlation (DIC) and scanning wide‐angle X‐ray diffraction (WAXD, with a narrow 10 µm square beam), this study maps local strain tensor properties and SIC in the vicinity of the crack tip and its peripheral zone (≈3 mm × 1 mm area). The analysis reveals a significant correlation between these properties. In the peripheral zone, there is a noticeable deviation of both the principal strain axis and the crystal orientation from the crack opening direction. These deviations are linearly correlated, which indicates that shear strain plays a significant role in determining the crystal orientation. Crucially, the maximum tensile component in the tensor of local principal strains predominantly dictates local crystallinity. This simplicity is attributed to the limited variation in types of deformation within the SIC region, with corresponding to deformations falling between planar and uniaxial stretching. These findings pave the way for predicting crystallinity distribution using solely strain field data, offering valuable insights into the role of SIC in enhancing the crack growth resistance of NR.