A novel type of superconducting joining technique has been introduced to join unreacted internal Mg diffusion (IMD) single-core MgB2 wires. Our method is based on fabricating a small diameter joint mould obtained by deforming an Nb/Cu composite tube with a longitudinal semi-cylindrical Mg and B core into a thick round wire. The small diameter of the joint provided advantages such as rapid cooling, low resistance, and the unique core design inside the joint ensured a uniform MgB2 phase formation. Scanning electron microscope analysis revealed that the IMD MgB2 wires had excellent contact with the superconducting MgB2 bulk material inside the joint. The joint resistance, calculated from the decay of the trapped magnetic field over time, is a quite low value of 6.44 × 10−16 Ω at 20 K. The transport critical current (Ic) of the joint is 62 A at 20 K under a self-magnetic field, and the n-value of the joint is 66 at 20 K under 1.5 T. The results showed that the Ic of our joint can be determined precisely, regardless of whether the magnetic field is applied from low to high or from high to low value during I–V measurements.
1 December 2012 in Radiation Physics and Chemistry
Lead-free SnIn solders are promising for superconducting magnet applications. However, their superconducting properties are not as good as lead solders. In order to improve the superconducting performance of the Sn–In solders, researchers have investigated the superconducting properties of ternary systems such as Sn–In–Bi for solder joints. In this study, powders of Pb, Nb, AgCu and grapheme nano pellets in the ratios of 0.5–5 wt% have been added into SnIn (35:65) to investigate their microstructural, thermal and superconducting properties. The added materials enhance the superconducting properties. We find that even low Pb additions show a dramatic improvement in superconducting properties, with an increase in both Tc and Jc values of up to 6.35 K and 1.47 × 104 A m−2, respectively. This shows that much lower Pb content superconducting solders can be effective and could be used to replace the PbBi solder commonly used with the superconducting properties Tc=8.4 K, HC2 = 1.77 T, HC = 0.0909 T.