The effect of using different electrolytes in the physical and optical properties of porous silicon was studied. To do this porous silicon (PS) samples photoluminescent in the visible range from (100) oriented n‐type crystalline silicon prepared by anodic etching were obtained. The first electrolyte was composed of a mixture of hydrofluoric acid (HF) and ethanol (CH3‐CH2‐OH) in a ratio of 1 : 2, respectively. The second was composed of hydrofluoric acid (HF), ethanol (CH3‐CH2‐OH), and hydrogen peroxide (H2O2) in a ratio of 1 : 1 : 2, respectively. Raman scattering, photoluminescence (PL), gravimetry, scanning electron microscopy (SEM), and energy dispersive spectrometer (EDS) measurements on the PSL were carried out. Raman scattering showed that the disorder in the samples obtained with H2O2 is greater than in the samples obtained without this. The PL from PS increased in intensity with the incremental change in the anodization time and showed a blueshift. The blueshift of PL is consistent with the reduction in size of the silicon nanocrystallites. The sizes of nanocrystals were estimated to be 3.08, 2.6, and 2.28 nm. The gravimetric analysis showed that the porosity increased with the incorporation of H2O2. SEM images (morphological analysis) showed an incremental change in the quantity and in the porous size.
Electroluminescent devices (ELD) based on junctions of indium doped zinc oxide (ZnO:In) and porous silicon layers (PSL) are presented in this work. PSL with different thicknesses and photoluminescent emission, around 680 nm, were obtained by anodic etching. PSL were coated with a ZnO:In film which was obtained by ultrasonic spray pyrolysis technique. Once obtained, this structure was optically and electrically characterized. When the devices were electrically polarized they showed stable electroluminescence (EL) which was presented as dots scattered over the surface. These dots can be seen with the naked eye. The observed EL goes from the 410 to 1100 nm, which is formed by different emission bands. The EL emission in the visible region was around 400 to 750 nm, and the emission corresponding to the infrared part covers the 750 to 1150 nm. The electrical characterization was carried out by current‐voltage curves (I-V) which show a rectifying behavior of the devices. Observed electroluminescent dots are associated with the electron‐hole injection into quantized states in PS as well as the emission from the ZnO:In film.
Because of the large surface area, optic properties and biocompatibility, porous silicon is a material with the potential to be applied in bio-delivery carriers and biosensors. In order to apply their properties as a biosensor substrate, gold nanoparticles were introduced in its structure. They also have a high surface area and optic features that added to the porous silicon properties will give the biosensor more sensitivity. One of the most used methods to obtain porous silicon/gold nanoparticles is metal salt-assisted chemical etching. Once these structures were obtained, porous silicon/Au nanoparticles were used as transducer to get a biogenic amine biosensor. The transducer was biofunctionalized through the introduction of functional groups on its surface by the absorption method. Scanning Electron Microscopy and X ray Energy Dispersive Spectroscopy showed the presence of gold in the porous silicon structure. Infrared spectrometry with Fourier Transform studies demonstrated the introduction of the elements of the biosensor. The optical detection of biogenic amine was based on the changes of the signals related to the reactions between the histamine and the recognized element used (diamine oxidase).
We present zinc oxide (ZnO) particles obtained inside a porous silicon matrix in the same electrolytic process using a p-type silicon wafer in a hydrofluoric acid (HF) solution containing formaldehyde (CH2O) and hydrated zinc sulfate as additives. The X-ray diffraction pattern of the sample confirmed the presence of ZnO with a hexagonal-type wurtzite structure. Photoluminescence (PL) spectra of the samples, before and after the functionalization process, were measured to observe the effect of ZnO inside the porous silicon. The PL measurements of porous silicon functionalized with ZnO (ZnO/PS) revealed infrared, red, blue, and ultraviolet emission bands. The ultraviolet region corresponds to the band-band emission of ZnO, and the visible emission is attributed to defects. The results of the nitrogen adsorption/desorption isotherms of the PS and ZnO/PS samples revealed larger BET surface areas and pore diameters for the ZnO/PS sample. We conclude that ZnO/PS can be obtained in a one-step electrolytic process. These types of samples can be used in gas sensors and photocatalysis.