Fast neutron imaging has a great potential as a nondestructive technique for testing large objects. The main factor limiting applications of this technique is detection technology, offering relatively poor spatial resolution of images and low detection efficiency, which results in very long exposure times. Therefore, research on development of scintillators for fast neutron imaging is of high importance. A comparison of the light output, gamma radiation sensitivity and spatial resolution of commercially available scintillator screens composed of PP/ZnS:Cu and PP/ZnS:Ag of different thicknesses are presented. The scintillators were provided by RC Tritec AG company and the test performed at the NECTAR facility located at the FRM II nuclear research reactor. It was shown that light output increases and the spatial resolution decreases with the scintillator thickness. Both compositions of the scintillating material provide similar light output, while the gamma sensitivity of PP/ZnS:Cu is significantly higher as compared to PP/ZnS:Ag-based scintillators. Moreover, we report which factors should be considered when choosing a scintillator and what are the limitations of the investigated types of scintillators.
The compound SrAl2O4:Eu2+,Dy3+ is currently one of the best‐performing persistent phosphors and numerous studies have been performed to understand the mechanisms involved in its afterglow process. One aspect which so far has received only limited attention is the dependence of loading curve characteristics on dopant concentrations. Herein, a detailed study of the loading curves of SrAl2O4:Eu2+,Dy3+ as a function of composition, sample temperature, and pump intensity is presented, completed by emission decay and quantum yield measurements. The observed emission decays can be described using the Inokuti−Hirayama equation for a Dexter energy transfer (ET) process. As the Dexter ET rate and the electron transfer rate have a similar radial dependence, the Inokuti−Hirayama equation can also describe the electron transfer process involved for the trapping process. These observations indicate that in this persistent phosphor, the trapping process is a local process; however, different types of traps appear to present different “Dexter” critical radii R0. This electron transfer is also temperature dependent, which requires further investigations.
16 April 2002 in European Journal of Organic Chemistry
We performed a study of the initial and long term light yield of different scintillation screen mixtures for neutron imaging during constant neutron irradiation. We evaluated the light yield during different neutron flux levels as well as at different temperatures. As high frame rate imaging is a topic of interest in the neutron imaging community, the decay characteristics of scintillation screens are of interest as well. Hence, we also present and discuss the decay behavior of the different scintillation screen mixtures on a time scale of seconds. We have found that the decay time of ZnS:Cu/6LiF excited with a high neutron flux is potentially much longer than typically stated. While most of the tested scintillation screens do not provide a significant improvement over currently used scintillation screen materials, Zn(Cd)S:Ag/6LiF seems to be a good candidate for high frame rate imaging due to its high light yield, long-term stability as well as fast decay compared to the other evaluated scintillation screens.
16 August 2005 in Journal of Physical Organic Chemistry