AZ91D Mg alloy was treated by ultrasonic surface rolling processing (USRP) and subsequent recovery treatment at different temperatures. The dry sliding friction test was performed to investigate the effects of USRP and subsequent recovery treatment on the wear resistance of AZ91D Mg alloy by a ball-on-plate tribometer. The microstructure, properties of plastic deformation layer and worn morphology were observed by optical microscope (OM), scanning electron microscope (SEM), transmission electron microscope (TEM), X-ray diffraction (XRD) analysis and microhardness tester. Results illustrate that the grains of AZ91D Mg alloy surface layer are refined to nanocrystallines. The maximum microhardness of the top surface of the USRP sample reaches 102.3 HV. When USRP samples are treated by recovery treatment at 150 °C, 200 °C and 250 °C, the microhardness of the top surface decreases to 90.68 HV, 79.29 HV and 75.06 HV, respectively. The friction coefficient (FC) and wear volume loss of the USRP-R-150 sample are the lowest among all the samples. The worn surface morphology of the USRP-R-150 sample is smoother than that of other samples, indicating that the wear resistance of AZ91D Mg alloy treated by USRP and recovery treatment at 150 °C is improved significantly.
Fatigue life prediction for the notched components is an essential step within the design process of machines. Fatigue strength and life prediction of 40Cr notched steel before and after shot peening were studied. Fatigue fracture of specimens treated by three shot peening intensity parameters was discussed. The life prediction considering residual stress, work hardening and surface roughness caused by shot peening was analyzed. The results indicated that fatigue strength was obviously improved after shot peening and the improvement effect was gradually enhanced with the increase of shot peening intensity. The predicted values based on Rz coefficient showed a good correspondence with the experimental data.
5 November 2018 in IOP Conference Series: Materials Science and Engineering
Based on Hastelloy C-276 sheet materials, the microstructure, element segregation and mechanical properties of weld joints were studied using pulse laser welding technology. It is noted that there are three morphological grains in the weld zone, which is columnar dendrites, cellular crystals and equiaxed grains, respectively. Compared with the base metal, the microstructure of the weld zone is obviously refined. Element segregation exists in the weld zone where no secondary phases formed. In addition, the microhardness of the weld joints is greater than that of the base metal by 12%. Its yield strength is equivalent to the yield strength of the base metal, and the tensile strength is 93% of that of the base metal. There are plenty of dimples in the fracture of the weld joints and the base metal, and the fracture modes of both are all ductile fracture.
Fatigue life tests and fatigue crack growth rate (FCGR) tests in the air and water environment were conducted on X80 pipeline steel welded joints (welded by CO2 arc welding). Scanning electron microscope (SEM) and electron backscatter diffraction (EBSD) were utilized to investigate the internal influential mechanisms of the water environment during fatigue crack initiation and propagation stages, respectively. Results show that a great many oxide particles induced by the water environment gradually formed the fatigue crack initiation site and decreased fatigue life of welded joints. Meanwhile, the preferred grain orientation of //ND and CSL boundaries of Σ3, Σ11, Σ13c, Σ17b, Σ25a, and Σ25b are both prone to fatigue propagation when loading in the water environment. In addition, a coalescence of the stress intensity factor (SIF) range and water environment accelerated FCGR by motivating secondary slip systems of {112} and {123} in bcc crystalline structures.
1 February 2020 in IOP Conference Series: Earth and Environmental Science
Laser welding is an ideal method to join hastelloy C-276 for the good characters. Presently, there are few studies on corrosion resistance of the weld joint of hatselloy C-276. The corrosion resistance of hastelloy C-276 pulse laser welded joints was studied in this paper. The results of the electrochemical testing both in neutral and acidic solution show that the corrosion resistance of the weld is better than the base metal. The microstructure was analyzed by using SEM, EDS and XRD, it is found that the grain of the weld obviously is refined and the size reduces to 2-5μm, which is benefit to the corrosion resistance, and slight micro-segregation of Mo occurs and no second phase formation in the weld which has little effect on the corrosion resistance. The change of the microstructure makes it that the corrosion resistance of the weld is superior to that of the base metal.