Yu Liu

Prof. Dr. Yu Liu

Jilin University

Research Focus & Metrics

Academic Career Length

12Years (2015-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
14 December 2020 in Materials
Verified
Journal Article
Open access
PDF file
XZXiaohui Zhao
Xiaohui Zhao
KLKaichao Liu
Kaichao Liu
DXDesheng Xu
Desheng Xu
YLYu Liu
Yu Liu
CHChunhua Hu
Chunhua Hu
AZ91D Mg alloy was treated by ultrasonic surface rolling processing (USRP) and subsequent recovery treatment at different temperatures. The dry sliding friction test was performed to investigate the effects of USRP and subsequent recovery treatment on the wear resistance of AZ91D Mg alloy by a ball-on-plate tribometer. The microstructure, properties of plastic deformation layer and worn morphology were observed by optical microscope (OM), scanning electron microscope (SEM), transmission electron microscope (TEM), X-ray diffraction (XRD) analysis and microhardness tester. Results illustrate that the grains of AZ91D Mg alloy surface layer are refined to nanocrystallines. The maximum microhardness of the top surface of the USRP sample reaches 102.3 HV. When USRP samples are treated by recovery treatment at 150 °C, 200 °C and 250 °C, the microhardness of the top surface decreases to 90.68 HV, 79.29 HV and 75.06 HV, respectively. The friction coefficient (FC) and wear volume loss of the USRP-R-150 sample are the lowest among all the samples. The worn surface morphology of the USRP-R-150 sample is smoother than that of other samples, indicating that the wear resistance of AZ91D Mg alloy treated by USRP and recovery treatment at 150 °C is improved significantly.

14 June 2016 in Materials
Verified
Journal Article
Open access
PDF file
XZXiaohui Zhao
Xiaohui Zhao
MWMingyi Wang
Mingyi Wang
ZZZhiqiang Zhang
Zhiqiang Zhang
YLYu Liu
Yu Liu
Ultrasonic peening treatment (UPT) as a method of severe plastic deformation was used to treat cruciform welded joints of Q345 steel. The application of UPT achieves material surface nanocrystallization of the peening zone, reduces stress concentration, and produces residual compressive stresses at the welded toe. Micro-structure, hardness, stress relief, S-N curve, and the fatigue fracture mechanism of cruciform welded joint of Q345 steel, both before and after UPT, were analyzed in detail. The main results show that: stress concentration and residual tensile stress are the main reasons to reduce fatigue strength of cruciform welded joints. The fatigue life of cruciform welded joints is improved for surface hardening, compressive stress, and grain refinement by UPT. Residual compressive stress caused by UPT is released with the increase of fatigue life. A very significant fatigue strength improvement happens when UPT is replenished repeatedly after a certain number of cycles.

24 September 2015 in Materials
Verified
Journal Article
Open access
PDF file
XZXiaohui Zhao
Xiaohui Zhao
FLFuyong Li
Fuyong Li
YLYu Liu
Yu Liu
YFYanjun Fan
Yanjun Fan
Hydraulic support is the main supporting equipment of the coal mining systems, and they are usually subjected to fatigue failure under the high dynamic load. The fracture positions are generally at welded joints where there is a serious stress concentration. In order to investigate and further improve the fatigue strength of hydraulic support, the present work first located the possible position where fatigue failure occurs through finite element analysis, and then fatigue tests were carried out on the different forms of welded joints for the dangerous parts. Finally, Fatigue strength-life (S-N) curves and fracture mechanism were studied. This research will provide a theoretical reference for the fatigue design of welded structures for hydraulic support.

20 February 2017 in Metals
Verified
Journal Article
Open access
PDF file
XZXiaohui Zhao
Xiaohui Zhao
YZYanjun Zhang
Yanjun Zhang
YLYu Liu
Yu Liu
High-frequency impacting and rolling was applied on AZ31B magnesium alloy to obtain a gradient nano-structured surface. Surface characteristics were experimentally investigated, and the nanocrystallization mechanism is discussed in detail. Results showed that the gradient nano-structure with the characteristics of work hardening, compressive residual stress and a smooth surface was induced on the treated surface. Grains on the top surface were generally refined to around 20 nm. Twins, dislocations and dynamic recrystallization dominated the grain refinement process. Fatigue strength of the treated specimens corresponding to 107 cycles was increased by 28.6% compared to that of the as-received specimens. The work hardened layer induced by high-frequency impacting and rolling is the major reason to improve fatigue life.

6 November 2022 in Sensors
Verified
Journal Article
Open access
PDF file
XZXiaohui Zhao
Xiaohui Zhao
YZYaowen Zhang
Yaowen Zhang
HWHao Wang
Hao Wang
YLYu Liu
Yu Liu
BZBao Zhang
Bao Zhang
SHShaoyang Hu
Shaoyang Hu
Real-time tracking welding with the assistance of structured light vision enhances the intelligence of robotic welding, which significantly shortens teaching time and guarantees accuracy for user-customized product welding. However, the robustness of most image processing algorithms is deficient during welding practice, and the security regime for tracking welding is not considered in most trajectory recognition and control algorithms. For these two problems, an adaptive feature extraction algorithm was proposed, which can accurately extract the seam center from the continuous, discontinuous or fluctuating laser stripes identified and located by the CNN model, while the prior model can quickly remove a large amount of noise and interference except the stripes, greatly improving the extraction accuracy and processing speed of the algorithm. Additionally, the embedded Pauta criterion was used to segmentally process the center point data stream and to cyclically eliminate outliers and further ensure the accuracy of the welding reference point. Experimental results showed that under the guarantee of the above-mentioned seam center point extraction and correction algorithms, the tracking average error was 0.1 mm, and even if abnormal trajectory points existed, they did not cause welding torch shaking, system interruption or other accidents.

29 December 2017 in Metals
Verified
Journal Article
Open access
PDF file
XZXiaohui Zhao
Xiaohui Zhao
GXGuilian Xue
Guilian Xue
YLYu Liu
Yu Liu
The dry sliding friction and wear behaviors of TC11 titanium alloy subjected to the ultrasonic impacting and rolling process (UIRP) were studied in the present work. The microstructure of the deformation layer and the morphology of the worn surfaces were observed. The results clearly show that the wear performance of TC11 alloy after UIRP is better than that of TC11 alloy before UIRP under the same testing conditions. This can be attributed to the gradient nanostructure, work hardening, and low surface roughness of the treated surface layer. For the untreated samples, wear resistance first decreases and then increases with the increase of the sliding speed. Both the friction coefficient (FC) and wear rate reach a maximum value at a sliding speed of 478 r/min, and the corresponding worn surface is the most serious. While for UIRP treated samples, better friction and wear behaviors are obtained at a sliding speed of 478 r/min. This is because the deformation layer plays a protective role against wear.