To address the issue of cracking in aluminum extrusion dies during operation, this study employs laser cladding technology to modify the surface of these dies. This modification aims to enhance their hardness and friction resistance. Laser cladding technology was utilized to coat the surface of H13 steel with Stellite 12, a cobalt-based alloy, at varying laser power levels. The surface formation quality, microstructural organization, phase composition, microhardness, and wear resistance of the coatings were investigated using optical microscopy, scanning electron microscopy, energy-dispersive spectroscopy, X-ray diffraction (XRD), microhardness testing, and confocal microscopy. The results indicated that as the laser power increased, the surface formation quality of the coating gradually improved, while the dilution rate of the coating increased. Changes in the phase composition and microstructure were not significant, and both microhardness and wear resistance initially increased before decreasing. Optimal process parameters for achieving good surface formation quality, high microhardness, and strong wear resistance were found to be a laser output power of 2200 W, scanning speed of 10 mm/s, feeding rate of 1.2 r/min, and overlap rate of 40%. The results indicate that the coating applied to the surface of H13 steel using Stellite 12 enhances the performance of aluminum extrusion dies.
Warm compression tests were carried out on low carbon and low alloy steel at temperatures of 600–850 °C and stain rates of 0.01–10 s−1. The evolution of microstructure and texture was studied using a scanning electron microscope and electron backscattered diffraction. The results indicated that cementite spheroidization occurred and greatly reduced at 750 °C due to a phase transformation. Dynamic recrystallization led to a transition from {112} texture to {111} texture. Below 800 °C, the intensity and variation of texture with deformation temperature is more significant than that above 800 °C. The contents of the {111} texture and {111} texture were equivalent above 800 °C, resulting in the better uniformity of γ-fiber texture. Nucleation of //ND-oriented grains increased, leading to the strengthening of //ND texture. Microstructure analysis revealed that the uniform and refined grains can be obtained after deformation at 800 °C and 850 °C. The texture variation reflected the fact that 800 °C was the critical value for temperature sensitivity of warm deformation. At a large strain rate, the lowest dislocation density appeared after deformation at 800 °C. Therefore, 800 °C is a suitable temperature for the warm forming application, where the investigated material is easy to deform and evolves into a uniform and refined microstructure.
Aluminum alloy is widely used in automobile parts because of its light weight and good process performance. In view of the complex structure of aluminum alloy automobile rear upper control arms, multiple forming processes and the difficulty in quality control, in this paper, we propose a rolling-forging composite process to produce a rear upper control arm. Based on the reasonable volume distribution of the blank by cross-wedge rolling, multi-step forging was carried out. Finite element simulation of thermomechanically coupled multi-step forming was carried out using DEFORM software. Based on a comparison of the traditional process and the proposed rolling-forging composite forming process, we concluded that the rolling-forging composite process can greatly reduce the material cost and the forming force, resulting in superior product performance. The coarse-grain structure of products at different process temperatures was analyzed by a crystal-phase experiment. The results show that the process temperature of the multi-step process, as well as the heat treatment temperature and time have an important influence on the coarse-grain structure of the product. The optimal preheating temperatures for preforging and final forging dies were determined to be 335 °C and 350 °C, respectively; a preheating temperature of 530 °C and a solution time of 45 min resulted in the least coarse-grain surface structure. The research results provide a theoretical basis for improving the multi-step forming quality of automobile rear upper control arms.