At present, the filling mining method is widely used. To study strength evolution laws of cemented tailings backfill (CTB) under different curing ages, in the experiment, mine tailings were used as aggregates, ordinary Portland cement (PC32.5) was used as cementing materials, and different additives (lime and fly ash) were added to make filling samples with the solids mass concentration at 74% and the cement-sand ratios 1:4, 1:6 and 1:8. Based on the nuclear magnetic resonance (NMR) technology, the porosity test of filling samples with curing ages of 3 d, 7 d and 28 d was carried out, and the uniaxial compressive strength test was carried out on the servo universal material testing machine. The relationship between the uniaxial compressive strength and porosity of backfills and the curing age in the three groups was studied, and change laws of the porosity variation and strength growth rate of backfills were analyzed. Based on the variation in porosity, the strength evolution model of the CTB under different curing ages was established, and the model was fitted and verified with test data. Results show that the uniaxial compressive strength, porosity, porosity variation, and strength growth rate of the three groups of backfills gradually increase with the increase of the curing age, the porosity of backfill basically increases with the decrease of the cement–sand ratio, and the porosity of backfill decreases with the increase of the curing age. Porosity variations and relative strength values of the three groups of backfills under different cement-sand ratios obey an exponential function, and the two have a good correlation, indicating that the established filling strength evolution model can well reflect strength evolution laws of the CTB with the change of curing age.
Freeze-thaw weathering changes the pore structure, permeability, and groundwater transportation of rock material. Meanwhile, the change in rock material structure deduced by frost heaving deteriorates mechanical properties of rock material, leading to instability and insecurity of mine slopes in cold regions. In this paper, rock-like specimens containing prefabricated cracks at different angles and having undergone various freeze-thaw cycles are used as the object. Their pore structure, compressive mechanical properties, strain energies, failure characteristics, and the connection between pore structure and mechanical properties are analyzed. Results show that the porosity, spectrum area of mesopores, and spectrum area of macropores increase with the increase in freeze-thaw cycles, while crack angle shows no obvious influence on pore structure. Peak stress and elastic modulus drop with the increase in freeze-thaw cycles, while peak strain shows an increasing trend. Peak stress and elastic modulus decrease in the beginning, and then increase with the increase in crack angle, while peak strain shows a reverse trend. Elastic strain energy and pre-peak strain energy drop with the increase in freeze-thaw cycles. Elastic strain energy decreases first, and then increases with the increase in crack angle. The correlation between the spectrum area of macropores and elastic modulus is the strongest among different pores. Elastic modulus and peak stress decrease with the increase in macropore spectrum area, and peak strain increases with the increase in macropore spectrum area.
Microscopic characteristics greatly affect mechanical and physical properties as they exert vital impact on the stability and durability of materials. In this paper, widely distributed sandstone was chosen as the research object. Sandstone was treated with a coupled effect of Freeze–Thaw (F–T) weathering and acid solution, where freeze–thaw cycles were set as 0, 10, 20, 30 and 40 cycles, and the pH of the acid solution were set as 2.8, 4.2, 5.6 and 7.0, respectively. Then, nuclear magnetic resonance was applied to measure the microscopic characteristics of sandstone, then porosity, pore size distribution and permeability before the fractal dimensions were obtained and calculated. Results show that porosity increases when F–T cycles increase, and its increase grows with the pH of acid solution decrease during the first 10 F–T cycles. Macro porosity, meso porosity and micro porosity account for the largest, second largest and smallest ratio of porosity growth. Meso porosity, micro porosity and macro porosity account for the largest, second largest and smallest ratio of total porosity. Permeability increases obviously with F–T cycle increase, while acid erosion exerts little influence on permeability increment overall. Fractal dimensions of meso pores and macro pores increase with F–T cycle increase overall, and they increase with pH decrease overall. Porosity has strong exponentially correlation with permeability. Fractal dimensions of meso pores and macro pores have good linearly correlation with permeability, while correlation between porosity and fractal dimensions are not that obvious.